Relay
A relay and oxide technology, applied in circuits, electrical switches, electrical components, etc., to achieve excellent welding performance, greatly reduce the amount of precious metals, and reduce costs.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] A relay, the contact adopts double-layer silver-based composite oxide electrical contact material, and the moving spring adopts reed composite material; the double-layer silver-based composite oxide electrical contact material includes two layers, one of which is AgCuZn layer, another layer is the compound oxide layer of silver, is fixed by fusing between two layers, wherein the preparation method of the compound oxide layer of silver comprises the following steps:
[0027] (1) Alloy smelting. Ag, Sn, La, Zr are mixed according to the following mass percentages and then smelted to form an alloy melt, wherein Sn is 10%, La is 1%, Zr is 5%, and the balance is Ag. The melting temperature 600°C;
[0028] (2) Gas atomization powder making, the alloy melt is atomized by high-pressure atomization equipment to make alloy powder, wherein the gas atomization pressure is 10MPa;
[0029] (3) isostatic pressing ingot, the alloy powder is processed into embryo ingot by isostatic pre...
Embodiment 2
[0040] A relay, the contact adopts double-layer silver-based composite oxide electrical contact material, and the moving spring adopts reed composite material; the double-layer silver-based composite oxide electrical contact material includes two layers, one of which is AgCuZn layer, another layer is the compound oxide layer of silver, is fixed by fusing between two layers, wherein the preparation method of the compound oxide layer of silver comprises the following steps:
[0041] (1) Alloy smelting. Ag, Sn, La, Zr are mixed according to the following mass percentages and then smelted to form an alloy melt, wherein Sn is 5%, La is 2%, Zr is 5%, and the balance is Ag. The melting temperature is 800°C;
[0042] (2) Gas atomization powder making, the alloy melt is atomized by high-pressure atomization equipment to make alloy powder, wherein the gas atomization pressure is 15MPa;
[0043] (3) isostatic pressing ingot, the alloy powder is processed into embryo ingot by isostatic p...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com