Embodiment 1
[0042] The leather care agent that present embodiment provides comprises:
[0043]
[0044] 1) Put cyclized rubber, lemon oil, silicone grease, tallow, olive oil and high-boiling liquid alcohol into reaction kettle A, heat to 90°C, and stir for two hours to prepare mixture A;
[0045] Preparation of mixture B: put emulsifier, water, and antioxidant into reaction kettle B, heat to 90° C., and stir for two hours to prepare mixture B.
[0046] 2) Slowly add the mixture B into the reaction kettle A, keep the temperature at 90°C, stir for 4 hours, then cool down to 35°C, and discharge to obtain the leather care agent.
Embodiment 2
[0048] The leather care agent that present embodiment provides comprises:
[0049]
[0050]
[0051] 1) Put cyclized rubber, lemon oil, silicone grease, tallow, olive oil and high-boiling liquid alcohol into reaction kettle A, heat to 90°C, and stir for two hours to prepare mixture A;
[0052] Preparation of mixture B: put emulsifier, water, and antioxidant into reaction kettle B, heat to 90° C., and stir for two hours to prepare mixture B.
[0053] 2) Slowly add the mixture B into the reaction kettle A, keep the temperature at 90°C, stir for 4 hours, then cool down to 35°C, and discharge to obtain the leather care agent.
Embodiment 3
[0055] The leather care agent that present embodiment provides comprises:
[0056]
[0057] 1) Put cyclized rubber, lemon oil, silicone grease, tallow, olive oil and high-boiling liquid alcohol into reaction kettle A, heat to 90°C, and stir for two hours to prepare mixture A;
[0058] Preparation of mixture B: put emulsifier, water, and antioxidant into reaction kettle B, heat to 90° C., and stir for two hours to prepare mixture B.
[0059] 2) Slowly add the mixture B into the reaction kettle A, keep the temperature at 90°C, stir for 4 hours, then cool down to 35°C, and discharge to obtain the leather care agent.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com