Natural-color cargo cleaning technology
A kind of goods and natural color technology, applied in the direction of dry cleaning fiber products, textiles and paper making, fiber processing, etc., can solve the problems of poor product effect, dirty finished products, long time, etc., and achieve washing cost savings, short washing time, and excellent wetting Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] 1) Deblueing: Dissolve the oxalic acid and add it to the foaming pool, heat it to 55°C and put it into the natural color goods to soak for 3.5 hours;
[0021] 2) Washing: Rinse the oxalic acid with clean water after deblueing the natural color goods;
[0022] 3) Decontamination and whitening: Add 2.5kg of GL cleaning agent to every 50kg of dry natural-colored goods, blend the GL cleaning agent in the washing tank and stir well, and put the washed oxalic acid-cleaned natural-colored goods in after the water is heated to 55°C And keep stirring, soak for 25 minutes;
[0023] 4) Washing: put the cleaned goods into the washing machine, and then rinse them with clean water until there is no GL detergent;
[0024] 5) Sizing: Add starch into the slurry tank and stir evenly, dehydrate the natural color goods and put them in the slurry tank for slurrying.
Embodiment 2
[0026] 1) Deblueing: Dissolve the oxalic acid and add it to the foaming pool, heat it to 60°C and put it into the natural color goods to soak for 4 hours;
[0027] 2) Washing: Rinse the oxalic acid with clean water after deblueing the natural color goods;
[0028] 3) Decontamination and whitening: Add 2.5kg of GL cleaning agent to every 50kg of dry natural-colored goods, blend the GL cleaning agent in the washing tank and stir evenly, and put the washed oxalic acid-cleaned natural-colored goods in after the water is heated to 60°C And keep stirring, soak for 30 minutes;
[0029] 4) Washing: put the cleaned goods into the washing machine, and then rinse them with clean water until there is no GL detergent;
[0030] 5) Sizing: Add starch into the slurry tank and stir evenly, dehydrate the natural color goods and put them in the slurry tank for slurrying.
Embodiment 3
[0032] 1) Deblueing: Dissolve oxalic acid and add it to the foaming pool, heat it to 65°C and soak the natural color goods for 4.5 hours;
[0033] 2) Washing: Rinse the oxalic acid with clean water after deblueing the natural color goods;
[0034] 3) Decontamination and whitening: add 2.5kg of GL cleaning agent to every 50kg of dry natural-colored goods, blend the GL cleaning agent in the washing tank and stir well, and put the washed oxalic acid-cleaned natural goods into the washing tank after the water is heated to 65°C And keep stirring, soak for 35 minutes;
[0035] 4) Washing: put the cleaned goods into the washing machine, and then rinse them with clean water until there is no GL detergent;
[0036] 5) Sizing: Add starch into the slurry tank and stir evenly, dehydrate the natural color goods and put them in the slurry tank for slurrying.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com