Method for preparing diesel oil for alpine regions with gas condensate and coal tar
A condensate oil technology in alpine regions, applied in the petroleum industry, liquid carbon-containing fuels, hydrocarbon distillation, etc., can solve the problems of incomplete replacement and achieve the effects of improving utilization value, increasing production, and sufficient raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0063] Special additives are prepared by the following methods, please refer to image 3 , the special additive preparation method comprises the following steps:
[0064] Step S300, placing the weighed fatty alcohol polyoxyethylene ether and oleic acid in a reactor with a stirring device under ambient pressure, wherein the ambient pressure refers to the natural atmospheric pressure in the area where the production facility is located;
[0065] Step S301, under stirring, slowly add naphthenate, petroleum ether and core additives, while keeping the temperature of the mixed material at 30-80°C, in which fatty alcohol polyoxyethylene ether, oleic acid, naphthenate, petroleum The weight percent of ether, core additive is:
[0066] Fatty alcohol polyoxyethylene ether 10-30%;
[0067] Oleic acid 10-20%;
[0068] Naphthenate 20-25%;
[0069] Petroleum ether 10-15%;
[0070] Core additives 10-40%;
[0071] In step S302, after all the materials are added, the heat preservation and...
Embodiment 1
[0084] The components of special additives and the percentage by weight of each component are:
[0085]
[0086]
[0087] Described core additive, its component and the weight percent of each component are:
[0088]
[0089] The special additive preparation method is as follows:
[0090] Under ambient pressure, place the weighed fatty alcohol polyoxyethylene ether and oleic acid in a reactor with a stirring device; under stirring, slowly add sodium naphthenate, petroleum ether and core additives while maintaining The temperature of the mixed material is 70°C; after adding all the materials, continue to keep warm and stir for 60 minutes, and discharge the material to obtain the special additive.
[0091] The preparation method of described core additive is as follows:
[0092] Under ambient pressure, place the weighed rapeseed sulfonated oil in a reaction kettle with a stirring device; under stirring, slowly add ferrocene, potassium chlorate, sodium sulfonate, diethy...
Embodiment 2
[0094] The components of special additives and the percentage by weight of each component are:
[0095]
[0096] Described core additive, its component and the weight percent of each component are:
[0097]
[0098] The preparation method of special additive is as follows:
[0099] Under ambient pressure, place the weighed fatty alcohol polyoxyethylene ether and oleic acid in a reactor with a stirring device; under stirring, slowly add barium naphthenate, petroleum ether and core additives, while maintaining The temperature of the mixed material is 70°C; after all the materials are added, continue to keep warm and stir for 40 minutes, and discharge the material to obtain the special additive.
[0100] The preparation method of described core additive is as follows:
[0101] Under ambient pressure, place the weighed linseed sulfonated oil in a reaction kettle with a stirring device; under stirring, slowly add ferrocene, potassium chlorate, barium sulfonate, triethylene ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com