A production process and technology of hirudin, which is applied in the directions of skin care preparations, cosmetics, cosmetic preparations, etc., can solve problems such as dull skin tone, and achieve the effects of enhancing skin elasticity, whitening, moisturizing, and rejuvenating skin, and improving blood circulation.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0064] (1) Wash the mixing pot, oil phase pot and water phase pot with purified water, and sterilize with 75% ethanol;
[0065] (2) Weigh 62.24kg of deionized water into the water phase pot, add 5kg of glycerol and 3kg of 1,3 propylene glycol, heat to 95°C for 20 minutes to sterilize, then add 0.2kg of acrylic acid copolymer and stir to dissolve; the temperature is controlled at 90°C, Add 5kg oat polypeptide, 3kg saffron extract, 1kg licorice brass, 1kg collagen polypeptide, 1kg caffeine derivative to the water phase;
[0066] (3) Heat the homogenizing pot to 85°C for later use;
[0067] (4) Put all the oil phase raw materials into the oil phase pot and heat to 85°C, then pump the oil phase into the homogenization pot, and keep the speed of the homogenization pot at 40r / min;
[0068] (5) Slowly pump the product obtained in step (2) into the homogeneous pot and stir and emulsify for 20 minutes;
[0069] (6) Keep the vacuum state, add 0.2kg triethanolamine, stir and emulsify f...
Embodiment 2
[0075] (1) Wash the mixing pot, oil phase pot and water phase pot with purified water, and sterilize with 75% ethanol;
[0076] (2) Weigh 60kg of deionized water and add it to the water phase pot, add 4kg of glycerol and 2kg1,3 propylene glycol, heat to 90°C for 22 minutes to sterilize, then add 0.3kg of acrylic acid copolymer and stir to dissolve; the temperature is controlled at 85°C. Add 6kg oat polypeptide, 2kg saffron extract, 0.5kg licorice brass, 1.5kg collagen polypeptide, 0.5kg caffeine derivative to the water phase;
[0077] (3) Heat the homogenizing pot to 80°C for later use;
[0078] (4) Put all the oil phase raw materials into the oil phase pot and heat to 90°C, then pump the oil phase into the homogenization pot, and keep the speed of the homogenization pot at 38r / min;
[0079] (5) Slowly pump the product obtained in step (2) into the homogeneous pot and stir and emulsify for 22 minutes;
[0080] (6) Keep the vacuum state, add 0.3kg triethanolamine, stir and em...
Embodiment 3
[0086] (1) Wash the mixing pot, oil phase pot and water phase pot with purified water, and sterilize with 75% ethanol;
[0087] (2) Weigh 64kg of deionized water and add it to the water phase pot, add 6kg of glycerol and 4kg1,3 propylene glycol, heat to 100°C for 18 minutes to sterilize, then add 0.1kg of acrylic acid copolymer and stir to dissolve; the temperature is controlled at 95°C. Add 4kg of oat polypeptide, 4kg of saffron extract, 1.5kg of licorice brass, 0.5kg of collagen polypeptide, and 1.5kg of caffeine derivatives to the water phase;
[0088] (3) Heat the homogenizing pot to 90°C for later use;
[0089] (4) Put all the oil phase raw materials into the oil phase pot and heat to 80°C, then pump the oil phase into the homogenization pot, and keep the speed of the homogenization pot at 42r / min;
[0090] (5) Slowly pump the product obtained in step (2) into the homogeneous pot and stir and emulsify for 18 minutes;
[0091] (6) Keep the vacuum state, add 0.1kg trietha...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com