A technology of thiazolphos and granules, which is applied in the field of thiazolphos-coated controlled-release granules, can solve the problems of crop injury, inconvenient operation, and the control effect cannot be kept constant for a long time, and achieve a long-lasting and constant control effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] Example 1: 10% Thiazophos coated controlled-release granules
[0031]In terms of weight percentage, take 10% of thiazolphos technical substance and 60% of diatomaceous earth, mix evenly, granulate in a granulator, and control the particle size to 0.5-2.0mm, and the obtained granules are dried and sieved.
[0032] The obtained particles are placed in a fluidized bed and blown into a fluidized state, and preheated so that the particles in the fluidized state are at 70°C. Then mix 20% cellulose and 6% sulfonated paraffin evenly, then add 4% cyclohexanone and mix thoroughly to form a coating fluid, and use a delivery pump to deliver the coating fluid to the pressure at a speed of 1000mL / h. At the nozzle of the atomization device of 0.4Mpa.
[0033] The atomized coating solution is sprayed onto the particles in a fluidized state, so that the coating solution and the pesticide particles are fully mixed, and the coating is evenly coated. The thickness of the coating is contro...
Embodiment 2
[0034] Example 2: 20% Thiazophos coated controlled-release granules
[0035] In terms of weight percentage, take 20% of thiazophos technical substance and 45% of kaolin, mix evenly, and granulate in a granulator, the particle size is controlled at 0.5-2.0mm, and the obtained granules are dried and sieved.
[0036] The obtained particles are placed in a fluidized bed and blown into a fluidized state, and preheated so that the particles in the fluidized state are at 70°C. Then mix 10% urea-formaldehyde resin and 20% paraffin evenly, then add 5% acetone and mix thoroughly to form a coating fluid, and use a delivery pump to transport the coating fluid to a pressure of 0.3Mpa at a speed of 800mL / h at the nozzle of the atomizer.
[0037] The atomized coating solution is sprayed onto the particles in a fluidized state, so that the coating solution and the pesticide particles are fully mixed, and the coating is evenly coated. The thickness of the coating is controlled at 0.1-0.5mm an...
Embodiment 3
[0038] Example 3: 40% Thiazophos coated controlled-release granules
[0039] In terms of weight percentage, take 40% of thiazolphos technical substance and 30% of clay, mix them uniformly, granulate in a granulator, control the particle size to 0.5-2.0mm, and dry and sieve the obtained granules.
[0040] The obtained particles are placed in a fluidized bed and blown into a fluidized state, and preheated so that the particles in the fluidized state are at 70°C. Then mix 17% cellulose and 9% petroleum resin evenly, then add 4% methyl ethyl ketone and mix thoroughly to form a coating solution, and use a delivery pump at a speed of 1200mL / h to transport the coating solution to a pressure of 0.5 Mpa at the nozzle of the atomizer.
[0041] The atomized coating solution is sprayed onto the particles in a fluidized state, so that the coating solution and the pesticide particles are fully mixed, and the coating is evenly coated. The thickness of the coating is controlled at 0.1-0.5mm ...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com