Papermaking chemical mechanical pulp presoak softener and preparation method thereof
A chemical machinery and softener technology, applied in the direction of adding inorganic compounds, can solve the problems of unsatisfactory product strength, heavy operation and maintenance workload, and unsatisfactory product strength, so as to shorten processing time, improve equipment efficiency, and use safely Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The papermaking chemi-mechanical pulp presoak softener of the present embodiment is formulated by the following raw materials in parts by weight: sodium dodecyl sulfonate 8kg, fatty alcohol polyoxyethylene ether (3 ether) 12kg, alkyl phosphate (also Name mercerizing penetrant OPE, purchased from Shanghai Auxiliary Factory) 7kg, 98wt% concentrated sulfuric acid 1.5kg, anhydrous sodium sulfate 2.2kg, water 69.3kg.
[0016] Its preparation method: (1) weigh the raw materials of each component according to the weight ratio; (2) heat the weighed 69.3kg water to 25°C; (3) add 1.5kg of 98wt% concentrated sulfuric acid to the water, Heat to 50°C; (4) Add 8kg of sodium dodecylsulfonate and 12kg of fatty alcohol polyoxyethylene ether (3 ether), heat to 50°C; (5) Add 2.2kg of anhydrous sodium sulfate and alkyl phosphate (also known as mercerizing penetrant OPE) 7kg, heated to 55 ° C, stirred for 50 minutes, and it was ready.
[0017] The papermaking chemimechanical pulp presoakin...
Embodiment 2
[0019] The papermaking chemi-mechanical pulp presoaking softener of the present embodiment is formulated by the following raw materials in parts by weight: sodium cetyl sulfonate 9kg, fatty alcohol polyoxyethylene ether (5 ether) 11kg, alkyl phosphate (also Mercerizing penetrant OPE) 8kg, 98wt% concentrated sulfuric acid 2.5kg, anhydrous sodium sulfate 2kg, water 67.5kg.
[0020] Its preparation method: (1) Weigh the raw materials of each component according to the weight ratio; (2) Heat the weighed 67.5kg water to 30°C; (3) Add 2.5kg of 98wt% concentrated sulfuric acid and heat to 50°C; (4) Add 9kg of sodium cetyl sulfonate and 11kg of fatty alcohol polyoxyethylene ether (5 ether), and heat to 50°C; (5) Add 2kg of anhydrous sodium sulfate and alkyl phosphate (also known as Mercerizing penetrant (OPE) 8kg, heated to 55°C, stirred for 55 minutes, ready to serve.
[0021] The papermaking chemical mechanical pulp presoaking softener in this example was tested by Heli Company of ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com