[0013] It is prepared from raw materials with the following weight fraction ratio: Portland cement: fly ash: water: water reducing agent: rust inhibitor: fine aggregate: coarse aggregate: boron-containing filler: metal filler = 0.65~0.75: 0.35~0.25:0.52~0.72:0.007~0.012:0.014~0.016:2.1~3.6:2.5~4.4:0.01~0.015:0.85~0.89, the fine aggregate is sand with a particle size of 0.15~4.75mm, the The coarse aggregate is crushed stone with a particle size of 4.75-19.00 mm, the boron-containing filler is colemanite with a particle size of 1.0 mm, and the metal filler is iron or steel particles with a particle size of 7 mm.
[0014] A preparation method of anti-radiation and anti-corrosion concrete is characterized in that it is prepared by the following process steps according to the raw materials:
[0015] (1) Add the formula amount of coarse and fine aggregates into the mixer, add 35% of the water, stir for 30~60s to make the aggregate absorb water to saturation;
[0016] (2) Add the am...
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com