Magnesia cement slurry for water plugging, leak plugging, and temporary plugging of oil and gas well reservoirs and its preparation method
A technology of oil and gas wells and cement slurry, which is applied in the direction of chemical instruments and methods, drilling compositions, etc., can solve problems such as leakage, and achieve the effects of reducing leakage and low sensitivity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] Weigh 100 parts by weight of active magnesium oxide, 1 part by weight of hydroxyethyl cellulose, 0.5 parts by weight of sodium octaborate, 6 parts by weight of sucrose, and 30 parts by weight of calcium carbonate dry-mixed into dry powder, measure 84 parts by weight of water, weigh 34 parts by weight Parts by weight of anhydrous magnesium chloride are dissolved in water. Then, put the aqueous solution in the mixing container, the stirrer rotates at a low speed (4000±200 rpm), and add the mixed dry powder within 15 seconds, cover the lid of the stirrer, and turn it at a high speed (12000±200 rpm). 500 rpm) and continue to stir for 35 seconds, the oil and gas well reservoir water plugging, plugging, temporary plugging and plugging magnesia cement slurry is ready.
Embodiment 2
[0032] Take 100 parts by weight of active magnesium oxide, 1 part by weight of carboxymethyl hydroxyethyl cellulose, 0.5 parts by weight of sodium tetraborate, 4 parts by weight of sucrose, and 10 parts by weight of calcium carbonate dry-mixed as dry powder, measure 84 parts by weight of water, Weigh 14 parts by weight of anhydrous magnesium chloride and 16 parts by weight of magnesium sulfate heptahydrate and dissolve them in water. Then, put the aqueous solution in the mixing container, the stirrer rotates at a low speed (4000±200 rpm), and add the mixed dry powder within 15 seconds, cover the lid of the stirrer, and turn it at a high speed (12000±200 rpm). 500 rpm) and continue to stir for 35 seconds, the oil and gas well reservoir water plugging, plugging, temporary plugging and plugging magnesia cement slurry is ready.
Embodiment 3
[0034]Weigh 100 parts by weight of active magnesium oxide, 1.5 parts by weight of hydroxyethyl cellulose, 1 part by weight of sodium tetraborate, 8 parts by weight of sodium pentaborate, 2 parts by weight of sucrose, and dry mix 190 parts by weight of calcium carbonate as dry powder, measure 84 Parts by weight of water, 3 parts by weight of ethoxylated sodium alkyl sulfate, 0.75 parts by weight of coconut oil aminopropyl betaine, 34 parts by weight of anhydrous magnesium chloride and 64 parts by weight of ammonium dihydrogen phosphate are dissolved in water. Then, put the aqueous solution in the mixing container, the stirrer rotates at a low speed (4000±200 rpm), and add the mixed dry powder within 15 seconds, cover the lid of the stirrer, and turn it at a high speed (12000±200 rpm). 500 rpm) and continue to stir for 35 seconds, the oil and gas well reservoir water plugging, plugging, temporary plugging and plugging magnesia cement slurry is ready.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com