Porous tantalum serving as medical metal implanted material and preparation method thereof
An implant material and porous tantalum technology, applied in the field of porous medical metal implant materials, can solve the problems of insufficient finished product purity, carbon skeleton residues, and reduced biological safety, and achieve improved ductility, simple process, and guaranteed biocompatibility. Effects of Sexuality and Biosecurity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] Example 1: Weigh 12.5 g of polyvinyl alcohol and put it into a container with 240 ml of distilled water; place it on an electric stove to heat and stir to make it into an aqueous solution of polyvinyl alcohol. Use a 200g balance to weigh 60g of tantalum powder with an average particle size of less than 43 microns and an oxygen content of less than 0.1%, add 50ml of cooled polyvinyl alcohol aqueous solution, stir and mix evenly, and make it into a tantalum powder slurry. Use 10×10×30mm porous polyurethane foam (average pore diameter is 0.48mm, density 0.025g / cm 3 , hardness 50°) into it and pour until the pores of the polyurethane foam are filled with the tantalum powder slurry, then use a clamp to take out the polyurethane foam filled with the tantalum powder slurry and put it into a porcelain plate. Dry in a vacuum drying oven at a drying temperature of 60° C., a drying time of 8 hours, and a vacuum degree of 1 Pa. Degreasing treatment: the vacuum degree is lower than...
Embodiment 2
[0039] Example 2: Weigh 10 g of polyvinyl alcohol and put it into a container with 200 ml of distilled water; place it on an electric stove to heat and stir to make it into an aqueous solution of polyvinyl alcohol. Use a 200g balance to weigh 40g of tantalum powder with an average particle size of less than 43 microns and an oxygen content of less than 0.1%, add 32ml of polyvinyl alcohol aqueous solution, stir and mix evenly, and make it into a tantalum powder slurry. Use 10×10×25mm porous polyurethane foam (average pore diameter is 0.56mm, density 0.030g / cm 3 , hardness 60°) into it and pour until the pores of the polyurethane foam are filled with the tantalum powder slurry, then use a clamp to take out the polyurethane foam filled with the tantalum powder slurry and put it into a porcelain plate. Dry in a vacuum drying oven at a drying temperature of 100°C for a drying time of 4 hours and maintain a vacuum of 10 -2 Pa. Degreasing treatment: vacuum degree 10 -4 Pa, tempera...
Embodiment 3
[0042] Example 3: Weigh 11 g of polyvinyl alcohol and put it into a container with 220 ml of distilled water; place it on an electric stove to heat and stir to make it into an aqueous solution of polyvinyl alcohol. Use a 200g balance to weigh 45g of tantalum powder with an average particle size of less than 43 microns and an oxygen content of less than 0.1%, add 36ml of polyvinyl alcohol aqueous solution, stir and mix evenly, and make it into a tantalum powder slurry. Use 8×8×25mm porous polyurethane foam (average pore diameter is 0.70mm, density 0.035g / cm 3 , hardness 70°) into it and pour until the pores of the polyurethane foam are filled with the tantalum powder slurry, then use a clamp to take out the polyurethane foam filled with the tantalum powder slurry and put it into a porcelain plate. Dry in a vacuum drying oven at a drying temperature of 80°C for a drying time of 6 hours and maintain a vacuum of 10 -1 Pa. Degreasing treatment: vacuum degree 10 -3 Pa, temperatur...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
pore size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com