[0012] An anti-wear additive for lubricating oil is composed of base oil, dispersant, nano-scale metal powder, pour point depressant and viscosity index improver. The base oil is a mixture of 150BS and 10 centistokes, and its weight ratio is 1:1. The dispersant is polyisobutylene bisimide, the nanoscale metal powder includes copper oxide powder, magnesium powder, manganese powder and chromium powder, the pour point depressant is polymethacrylate, and the viscosity index improver is ethylene propylene copolymer (OCP ), its weight share ratio is 77% of base oil; 3% of dispersant; 6% of copper oxide powder; 6% of magnesium powder; 1.5% of manganese powder; 1% of chromium powder; Measure the above-mentioned base oil, dispersant, copper oxide powder, magnesium powder, manganese powder, chromium powder, pour point depressant and viscosity index improver according to the weight of each component, then mix evenly, heat and control the temperature at 50-60 ℃, stirred for 180 minutes, a...
example 2
[0018] An anti-wear additive for lubricating oil is composed of base oil, dispersant, nano-scale metal powder, pour point depressant and viscosity index improver. The base oil is a mixture of 150BS and 10 centistokes, and its weight ratio is 1:1. The dispersant is polyisobutylene bisimide, the nanoscale metal powder includes copper oxide powder, magnesium powder, manganese powder and chromium powder, the pour point depressant is polymethacrylate, and the viscosity index improver is ethylene propylene copolymer (OCP ), its weight share ratio is 74% of base oil; 4% of dispersant; 7% of copper oxide powder; 7% of magnesium powder; 2% of manganese powder; 1% of chromium powder; Measure the above-mentioned base oil, dispersant, copper oxide powder, magnesium powder, manganese powder, chromium powder, pour point depressant and viscosity index improver according to the weight of each component, then mix evenly, heat and control the temperature at 50-60 ℃, stirred for 240 minutes, and...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com