Sand wall sand textured architectural coating and production technology thereof
An architectural coating and sand-wall-shaped technology, which is applied in the field of sand-wall-shaped architectural coatings and its production technology, can solve the problems of poor stone imitation effect, water absorption, whitening, and stain resistance, and achieves good freeze-thaw resistance and rich texture. , the effect of preventing erosion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] In the present invention, first put 37.25% water and 1.5‰ thickener into the blender and stir evenly; then add 12% binder into the blender and stir evenly at high speed; then add 5‰ mixing aid into the blender and stir at low speed , stir it evenly, then add 50% colored sand and stir evenly at high speed; finally, add 1‰ antifungal agent into the mixer and stir until completely mixed, and the finished product can be finished by discharging and filling. The time of each stirring is generally 5-10 minutes, the speed at high speed is 1500r / min, and the speed at low speed is 300r / min.
[0021] The above-mentioned binder is a synthetic resin or a synthetic resin emulsion, wherein the synthetic resin emulsion is a silicone acrylic emulsion KD9, which has a silane group in terms of adhesion, so it has particularly good adhesion to inorganic substrates and is weather-resistant Excellent stain resistance; in terms of stain resistance, due to the presence of silane groups, it can...
Embodiment 2
[0028] First, put 18.075% water and 2.25‰ thickener into the mixer and stir evenly; then add 18.5% binder to the mixer and stir evenly at high speed; then add 5.5‰ mixing aid to the mixer and stir at a low speed. After it is stirred evenly, add 62.5% colored sand and stir evenly at high speed; finally, add 1.5‰ antifungal agent into the mixer and stir until it is completely mixed, and then discharge and fill it to become a finished product. Others are the same as those in Embodiment 1, and will not be repeated here.
Embodiment 3
[0030] First, put 14.89% water and 3‰ thickener into the mixer and stir evenly; then add 20% binder to the mixer and stir evenly at high speed; then add 6‰ mixing aid to the mixer and stir at low speed. After it is stirred evenly, add 65% colored sand and stir evenly at high speed; finally, add 2‰ antifungal agent into the mixer and stir until it is completely mixed, and then discharge and fill it to become a finished product. Others are the same as those in Embodiment 1, and will not be repeated here.
[0031] The spraying effect of the sand-wall-shaped architectural paint described in the present invention is solemn and elegant, comparable to stone materials, and can fully display the rich texture of natural stone materials. Sand wall-like architectural coatings have the characteristics of high hardness, rich texture, low cost, fire prevention, waterproof, acid and alkali resistance, pollution resistance, non-toxic, odorless, strong adhesion, and never fade. The long-term a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com