Embodiment 1
[0030] Embodiment 1: Novel ecological synergistic conditioning agent
[0031] The production method of amino acid polymer is to mix asparagine (ASN), glycine (GLY), methionine (MET) and lysine (LYB) uniformly according to 10:1:1:1 (molar ratio), and take 180 kg Add it into a 500L electrothermal rotary condensation reactor, heat it at 215°C for 5.5 hours, obtain 135 kg of reaction product after cooling, measure its molecular weight with a viscosity method to be 18700, put the reaction product into a stainless steel reactor, and add 54 kg of potassium hydroxide ( KOH), the temperature was raised to 70° C., reacted for 3 hours, and the pH value was adjusted to 9.5 to obtain 342 kilograms of amino acid polymers with a weight ratio of 40%.
[0032] Adsorbent mixing is premixing bentonite and peat at a weight ratio of 5:1.
[0033] The amino acid polymer finally obtained by the reaction is mixed with the adsorbent at a weight ratio of 1:20, and after uniformity, a binder is added f...
Embodiment 2
[0034] Embodiment 2: Novel ecological synergistic conditioning agent
[0035] The production method of amino acid polymer is to mix glutamic acid (GLU), leucine (LEU), tyrosine (TYR) and tryptophan (TRY) uniformly according to 12:1:1:1 (molar ratio) 180 kg was added to a 500L electrothermal rotary condensation reactor, heated at 215°C for 5.5 hours, and 127 kg of reaction product was obtained after cooling, whose molecular weight was 7700 as determined by viscosity method.
[0036] Adsorbent mixing is to pre-mix fly ash and sepiolite at a weight ratio of 5:1.
[0037] The amino acid polymer finally obtained by the reaction is mixed with the adsorbent at a weight ratio of 1:2, and after uniformity, a binder is added for granulation, and the finished product is obtained after drying and passing the inspection.
Embodiment 3
[0038] Embodiment 3: Novel ecological synergistic conditioning agent
[0039] The production method of amino acid polymer is that after arginine (ARG), serine (SER), valine (VAL), proline (PRO) are mixed uniformly by 10:1:1:2 (molar ratio), take 180 kg was added to a 500L electrothermal rotary condensation reactor, heated at 215°C for 5.5 hours, and 127 kg of reaction product was obtained after cooling, whose molecular weight was 1500 as determined by viscosity method.
[0040] Adsorbent mixing is to pre-mix medical stone and rare earth in a weight ratio of 20:1.
[0041] The amino acid polymer and the adsorbent are mixed twice according to the weight ratio of 10:1, and the finished product is obtained after uniform drying and inspection.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com