Decorating plate brick producing process
A production process and technology for slab tiles, which are applied in the field of production technology of decorative slab tiles made of glass, can solve the problems of easy-wearing background color, uneven surface and high cost, and achieve a strong sense of three-dimensional layering, good transparency and tightness. good effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] (1) Edge grinding, grinding, polishing, cleaning, and pressing of protective film on glass bricks;
[0020] (2) Spray one deck of epoxy resin varnish uniformly on one surface of the glass brick;
[0021] (3) Evenly spread a layer of laser powder on the upper layer of the epoxy resin varnish, sweep and press on the laser powder with a row sweep, so that the laser powder is evenly attached to the glass brick, and stand until the epoxy varnish is dry;
[0022] (4) Spray the primer on the upper layer of the laser powder sheet, then bake at 150°C for 30 minutes, and cool;
[0023] (5) Use plastic printing to print the base screen paint on the base paint, and wait for it to dry or dry to obtain decorative tiles.
Embodiment 2
[0025] (1) Edge grinding, grinding, polishing, cleaning, and pressing of protective film on glass bricks;
[0026] (2) Use a plastic screen to print the pattern of the laser powder paste on the glass brick, bake at a temperature of 150°C for 45 minutes, and cool;
[0027] (3) Spray a layer of epoxy resin varnish evenly on one surface of the glass brick;
[0028] (4) Evenly spread a layer of laser powder on the upper layer of the epoxy resin varnish, sweep and press on the laser powder with a row sweeper, so that the laser powder is evenly attached to the glass brick, and stand until the epoxy resin varnish is dry;
[0029] (5) Spray the primer on the upper layer of the laser powder sheet, then bake at 150°C for 30 minutes, and cool;
[0030] (6) Use plastic printing to print the base screen paint on the base paint, and wait for it to dry or dry to obtain decorative tiles.
Embodiment 3
[0032] (1) Edge grinding, grinding, polishing, cleaning, and pressing of protective film on glass bricks;
[0033] (2) Use a plastic screen to print the pattern of the laser powder paste on the glass brick, bake at a temperature of 150°C for 30 minutes, and cool;
[0034] (3) Spray a layer of epoxy resin varnish evenly on one surface of the glass brick;
[0035] (4) Evenly spread a layer of laser powder on the upper layer of the epoxy resin varnish, sweep and press on the laser powder with a row sweeper, so that the laser powder is evenly attached to the glass brick, and stand until the epoxy resin varnish is dry;
[0036] (5) Spray the primer on the upper layer of the laser powder sheet, then bake at 150°C for 60 minutes, and cool;
[0037] (6) Use plastic printing to print the base screen paint on the base paint, and wait for it to dry or dry to obtain decorative tiles.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com