High concentration sludge coal slurry and method for preparing the same
A high-concentration, sludge technology, applied in the petroleum industry, liquid carbon-containing fuel, fuel, etc., can solve the problems of increasing the process cost of sludge and coal slurry, and achieve the effects of low cost, low energy consumption and simple operation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] 1. Raw material
[0028] (1) Sewage sludge produced by a sewage treatment plant in Shanghai, water content ------80%, weight;
[0029] (2) Lump coal from a coal mine, water content ------ 2%, ash content ------ 15%;
[0030] (3) Additive (sodium lignosulfonate)
[0031] (4) Sludge modifier (calcium carbonate)
[0032] (5) Tap water
[0033] 2. Preparation conditions
[0034] (1) Raw material ratio (parts by weight)
[0035] 100 parts of coal, 25 parts of hydrous sludge, 45 parts of water, 1 part of additive, and 1 part of sludge modifier.
[0036] (2) Preparation method
[0037] Firstly, the sewage sludge is fully mixed with the sludge modifying agent, and left for 4 hours to obtain the modified sludge. Then grind and mix the modified sludge, coal, water and additives to make a high-concentration sludge-coal slurry
[0038] 3. Product performance indicators
[0039] (1) Appearance shape --- gray black paste. At 25°C, the apparent viscosity is below 1000mPa·s, ...
Embodiment 2
[0045] 1. Raw material
[0046] (1) Sewage sludge produced by a sewage treatment plant in Shanghai, water content ------80%, weight;
[0047] (2) Lump coal from a coal mine, water content ------ 2%, ash content ------ 8%;
[0048] (3) Additive (sodium methylnaphthalenesulfonate formaldehyde condensate)
[0049] (4) Sludge modifier (calcium hydroxide)
[0050] (5) Tap water
[0051] 2. Preparation conditions
[0052] (1) Raw material ratio (parts by weight)
[0053] 150 parts of coal, 45 parts of hydrous sludge, 58 parts of water, 1.5 parts of additives, and 1 part of sludge modifier.
[0054] (2) Preparation method
[0055] First, the sewage sludge is fully mixed with the sludge modifying agent, and left for 3 days to obtain the modified sludge. Then grind and mix the modified sludge, coal, water and additives to make a high-concentration sludge-coal slurry
[0056] 3. Product performance indicators
[0057] (1) Appearance shape --- gray black paste. At 25°C, the app...
PUM
Property | Measurement | Unit |
---|---|---|
Apparent viscosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com