[0036] Below in conjunction with embodiment, the present invention will be further described:
[0037] 1. Natural mineral licking brick additive ingredients, including the following components by weight percentage: 40% attapulgite clay, 20% bentonite, 20% zeolite, 12% medical stone and 8% shell, mixed evenly to form a mineral mixture.
[0038] 2. Grinding: Grinding the mineral mixture after batching, the particle size is ≤2mm.
[0039] 3. Sulfuric acid acidification treatment:
[0040] 1. The preparation of dilute sulfuric acid includes the following components by weight percentage: 4% of sulfuric acid with a concentration of 98%, 96% of water; 2. The batching of acidification treatment includes the following components by weight percentage: mineral mixture 55%, dilute sulfuric acid 45%; Transport the pulverized mineral mixture to the acidification tank, slowly add dilute sulfuric acid, and carry out acidification treatment at room temperature for 24 hours.
[0041] 4. High-...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com