A refined salt and new process technology, applied in the field of refined salt production, can solve the problems of refined salt agglomeration, which is difficult to obtain the desired effect, and achieve the effects of fast dissolution, high moisture absorption capacity, and reduced contact points
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0009] Sodium ferrocyanide was added to the refined saturated brine, pH = 7, so that the concentration was 1.0 mg / L. Put it into a glass-made natural circulation evaporation crystallizer for evaporation and concentration. The capacity of the material liquid in the evaporation crystallizer is 10 liters, the evaporation intensity is 0.39 kg of water / hour·liter, and the pressure of the evaporation chamber of the evaporation crystallizer is 79.5KPa (vacuum degree). The liquid temperature is 68°C. When there is salt to separate out, start feeding continuously, discharge salt intermittently, feeding speed is 9 liters / hour, slurry concentration 8%. After dehalogenation, rinsing and drying, the discharged wet salt is refined salt with a sodium ferrocyanide content of 9.0 mg / kg in the crystal form of concave cubes and star-shaped dendrites, and the product volume density is 0.70 g / kg cubic centimeters.
Embodiment 2
[0011] Sodium ferrocyanide was added to the refined saturated brine, pH = 8, so that the concentration was 2.0 mg / L. Put it into a glass-made natural circulation evaporation crystallizer for evaporation and concentration. The capacity of the material liquid in the evaporation crystallizer is 10 liters, the evaporation intensity is 0.30 kg water / hour·liter, and the pressure of the evaporation chamber of the evaporation crystallizer is -10.4KPa (gauge pressure). The feed liquid temperature is 105°C. When there is salt to separate out, start to feed continuously, discharge salt intermittently, feed rate is 3 liters / hour, slurry concentration 7%. After dehalogenation, rinsing and drying, the discharged wet salt is refined salt with a sodium ferrocyanide content of 7.5 mg / kg in the crystal form of concave cubes and star-shaped dendrites, and the product volume density is 1.0 g / kg cubic centimeters.
Embodiment 3
[0013] Potassium ferrocyanide was added to the refined saturated brine, pH = 9, to make the concentration 3.0 mg / L. Put it into a steel forced circulation evaporation crystallizer for evaporation and concentration. The capacity of the material liquid in the evaporation crystallizer is 300 liters, the evaporation intensity is 0.4 tons of water / hour·cubic meter, and the pressure of the evaporation chamber of the evaporation crystallizer is 82.3KPa (vacuum degree). The feed liquid temperature is 67°C. When there is salt to separate out, start to feed continuously, discharge salt intermittently, feed speed is 80 liters / hour, slurry concentration 9%. After dehalogenation, rinsing and drying, the discharged wet salt is a refined salt product with a potassium ferrocyanide content of 7.6 mg / kg in the form of concave cubes and star-shaped dendrites, and the volume density of the product is 0.82 grams. / cubic centimeter.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com