Natural latex preservative and concentrated natural latex prepared by using same
A technology of natural latex and preservatives, applied in the field of concentrated natural latex and natural latex preservatives, which can solve the problems of large fluctuations in mechanical stability, low chemical stability, and high cost of preservatives, and achieve small fluctuations in mechanical stability and chemical stability High durability and excellent preservation effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Field latex is essentially an alkaline colloid, and its pH value > 9 can keep the colloid stable for a long time; field natural latex is also a good biochemical material, which is easily eroded by microorganisms in the rubber plantation environment and produces volatile fatty acids, resulting in Its pH value drops rapidly, which seriously damages the stability of latex and directly affects the production of concentrated natural latex. For a long time, ammonia water has been used as its preservative in production, so that the ammonia content of latex can reach about 0.20%, so as to achieve the purpose of preservation.
[0019] The present embodiment provides a natural rubber latex preservative, the specific formula is as follows: it is formed by mixing potassium hydroxide solution, potassium laurate solution, dithiotetramethylthiuram and zinc oxide dispersion. Tetramethylthiuram and zinc oxide dispersion is a liquid obtained by grinding dithiotetramethylthiuram, zinc oxi...
Embodiment 2
[0021] Optimized on the basis of Example 1.
[0022] Weigh the field latex produced in Tunchang, Hainan in May, take 3kg at 11 o'clock noon, add natural latex preservative, and the added quality is 1.8% of the latex amount. The sample number is C.
[0023] The preparation of natural latex preservative: described natural latex preservative is mixed by potassium hydroxide solution, potassium laurate solution and dithiotetramethylthiuram and zinc oxide dispersion (liquid), in dry basis: The amounts of potassium hydroxide, potassium laurate, dithiotetramethylthiuram and zinc oxide relative to the latex are respectively: potassium hydroxide 0.18%, dithiotetramethylthiuram and zinc oxide total 0.06% by mass, 0.03% potassium laurate. Weigh and mix the above three liquids respectively, and calibrate their alkalinity (pH ≥ 14) before use.
[0024] The preparation process of solution and dispersion is:
[0025] Potassium hydroxide solution preparation: Take 20 parts of potassium hyd...
Embodiment 3
[0033] Optimized on the basis of Example 1.
[0034] Take 3 kg of field latex produced in August in Tunchang County, add natural latex preservative (the preparation method and proportion are the same as in Example 2), the added amount is 1.8% of the latex mass, and the sample number is d.
PUM
Property | Measurement | Unit |
---|---|---|
chemical stability | aaaaa | aaaaa |
chemical stability | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com