preparation example Construction
[0041] A preparation method of low-conductivity coolant, comprising the following steps:
[0042] A. Prepare deionized water, test its conductivity to ensure that it meets the requirements of first-grade water, and mix qualified deionized water with ethylene glycol under the condition of 20-60°C, and stir for 10-30 minutes to form solution 1;
[0043] B: Mix the polyether, polytricarboxylic acid and dicarboxylic acid in the multi-effect composite preservative according to a certain ratio at 50-70°C, and stir for 30-60 minutes;
[0044] C: At 50-70°C, add multi-effect compound preservative and defoamer to solution 1 and stir for 30-60 minutes to form solution 3;
[0045] D: Filter solution 3 through a cation exchange resin to obtain the product.
Embodiment 1
[0047] Embodiment 1, a kind of low-conductivity cooling liquid, comprises the raw material of following parts by weight (this embodiment is in gram):
[0048] Deionized water 50, ethylene glycol 50, multi-effect compound preservative 0.02, defoamer (EX-504) 0.001; among them, the multi-effect compound preservative is polyether, polytricarboxylic acid, sebacic acid according to 1: 0.1:1 mixed; the polyether structure is:
[0049]
[0050] The polytricarboxylic acid structure is:
[0051]
[0052] A preparation method of low-conductivity coolant, comprising the following steps:
[0053] A: Prepare deionized water, test its conductivity to ensure that it meets the requirements of first-class water, mix 50 grams of deionized water and 50 grams of ethylene glycol at 25 ° C, and stir for 30 minutes to form solution 1;
[0054] B: At 50°C, mix 0.02 grams of multi-effect preservative, in which polyether, polytricarboxylic acid, and sebacic acid are mixed at a ratio of 1:0.1:1, a...
Embodiment 2
[0061] Embodiment 2, a kind of low-conductivity coolant, comprises the raw material of following parts by weight (this embodiment is in gram):
[0062] Deionized water 10, ethylene glycol 90, multi-effect compound preservative 10, defoamer (CK-C155) 0.005; among them, the multi-effect compound preservative is polyether, polytricarboxylic acid, octadecanedioic acid Made by mixing 1:0.1:1;
[0063] The polyether structure is:
[0064]
[0065] The polytricarboxylic acid structure is:
[0066]
[0067] A preparation method of low-conductivity coolant, comprising the following steps:
[0068] A: Prepare deionized water, test its conductivity to ensure that it meets the requirements of first-class water, mix 10 grams of deionized water with 90 grams of ethylene glycol at 60 ° C, and stir for 10 minutes to form solution 1;
[0069] B: At 70°C, mix 10 grams of multi-effect preservative, in which polyether, polytricarboxylic acid, and octadecanedioic acid are mixed in a ratio...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com