Rail transit derailment valve casting process
A casting process and rail transportation technology, applied in the field of rail transportation, can solve the problems of inconvenient casting of materials, inconvenience of users, and easy quality problems, etc., and achieve the effects of eliminating casting stress, increasing performance, and facilitating processing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] Embodiment 1: a rail transit derailment valve casting process, comprising the following steps:
[0021] 1) Raw material preparation: purchase raw materials that meet the national standards, remove impurities from the purchased raw materials, and then put them into the melting device for melting treatment to form liquid metal. The melting temperature is 200 degrees Celsius;
[0022] 2) Forging molding: pour the liquid metal into the corresponding forging mold, wait until the liquid metal is solidified and formed, and get a preliminary part with a certain shape, and then stamp the preliminary part under the punching machine, and use a special stamping die for stamping , after the stamping is completed, the parts blanks of each part of the derailment valve are obtained;
[0023] 3) Heat treatment: heat the part blank to an appropriate temperature above the critical point AC3, and then cool it in the air after keeping it for an hour and a half. When the cooling is completed...
Embodiment 2
[0028] Embodiment 2: A rail transit derailment valve casting process, comprising the following steps:
[0029] 1) Raw material preparation: purchase raw materials that meet the national standards, remove impurities from the purchased raw materials, and then put them into the melting device for melting treatment to form liquid metal. The melting temperature is 230 degrees Celsius;
[0030] 2) Forging molding: pour the liquid metal into the corresponding forging mold, wait until the liquid metal is solidified and formed, and get a preliminary part with a certain shape, and then stamp the preliminary part under the punching machine, and use a special stamping die for stamping , after the stamping is completed, the parts blanks of each part of the derailment valve are obtained;
[0031] 3) Heat treatment: heat the part blank to an appropriate temperature above the critical point ACM, and then cool it in the air after keeping it for 70 minutes. When the cooling is completed, heat t...
Embodiment 3
[0036] Embodiment three: a rail transit derailment valve casting process, comprising the following steps:
[0037]1) Raw material preparation: Purchase raw materials that meet the national standards, remove impurities from the purchased raw materials, and then put them into the melting device for melting treatment to form liquid metal. The melting temperature is 180 degrees Celsius;
[0038] 2) Forging molding: pour the liquid metal into the corresponding forging mold, wait until the liquid metal is solidified and formed, and get a preliminary part with a certain shape, and then stamp the preliminary part under the punching machine, and use a special stamping die for stamping , after the stamping is completed, the parts blanks of each part of the derailment valve are obtained;
[0039] 3) Heat treatment: heat the part blank to an appropriate temperature above the critical point ACM, and then cool it in the air after keeping it for one hour. When the cooling is completed, heat ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com