Phenyl salicylate anti-ultraviolet blended yarn and production process thereof
A technology of phenyl salicylate and blended yarn, which is applied in the direction of yarn, textiles, papermaking, fiber treatment, etc. It can solve the problems of no processing technology and no anti-ultraviolet performance of hemp blended fabrics, and achieve good anti-ultraviolet performance, The effect of good elasticity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] The object of the invention is to provide an anti-ultraviolet blended yarn, which comprises the following components by weight: 40 parts of cotton fiber, 50 parts of spandex fiber and 10 parts of bamboo fiber.
[0027] The surface of the cotton fiber is provided with a layer of phenyl salicylate ultraviolet absorber.
[0028] The fineness of the cotton fiber is 76S.
[0029] Its production process comprises the following steps:
[0030] Step 1, pretreatment, opening;
[0031] Step 2, immerse the cotton fiber in the phenyl salicylate ultraviolet absorber at 50 DEG C for 3 hours, then take it out and dry it to make the cotton fiber with the phenyl salicylate ultraviolet absorber on the surface;
[0032] Cotton fibers and spandex fibers made in step 3 and step 2 are mixed in a "sandwich" type of layering according to the blending ratio;
[0033] Step 4, opening and cleaning process: the cotton fiber and spandex fiber mixed in the layer in step 3 are sequentially passed ...
Embodiment 2
[0045] The object of the invention is to provide an anti-ultraviolet blended yarn, which comprises the following components by weight: 55 parts of cotton fiber, 37 parts of spandex fiber and 8 parts of bamboo fiber.
[0046] The surface of the cotton fiber is provided with a layer of phenyl salicylate ultraviolet absorber.
[0047] The fineness of the cotton fiber is 80S.
[0048] Its production process comprises the following steps:
[0049] Step 1, pretreatment, opening;
[0050] Step 2, immerse the cotton fiber in the phenyl salicylate ultraviolet absorber at 50 DEG C for 3 hours, then take it out and dry it to make the cotton fiber with the phenyl salicylate ultraviolet absorber on the surface;
[0051] Cotton fibers and spandex fibers made in step 3 and step 2 are mixed in a "sandwich" type of layering according to the blending ratio;
[0052] Step 4, opening and cleaning process: the cotton fiber and spandex fiber mixed in the layer in step 3 are sequentially passed t...
Embodiment 3
[0064] The object of the invention is to provide an anti-ultraviolet blended yarn, which comprises the following components by weight: 75 parts of cotton fiber, 20 parts of spandex fiber and 5 parts of bamboo fiber.
[0065] The surface of the cotton fiber is provided with a layer of phenyl salicylate ultraviolet absorber.
[0066] The fineness of the cotton fiber is 89S.
[0067] Its production process comprises the following steps:
[0068] Step 1, pretreatment, opening;
[0069] Step 2, immerse the cotton fiber in the phenyl salicylate ultraviolet absorber at 50 DEG C for 3 hours, then take it out and dry it to make the cotton fiber with the phenyl salicylate ultraviolet absorber on the surface;
[0070] Cotton fibers and spandex fibers made in step 3 and step 2 are mixed in a "sandwich" type of layering according to the blending ratio;
[0071] Step 4, opening and cleaning process: the cotton fiber and spandex fiber mixed in the layer in step 3 are sequentially passed t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com