Aluminum-free lining paper for cigarettes and processing technology of aluminum-free lining paper
A processing technology and lining paper technology, applied in the directions of wrapping paper, wrapping paper, flexible covering, etc., can solve the problems of dullness, pollution, monotonous color, etc., and achieve the effect of good appearance effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] The processing technology of aluminum-free lining paper for cigarettes includes the following steps:
[0036] The surface smoothness of the base paper is 205s, which is greater than 200s, and can be used directly without treatment;
[0037] Print yellow ink on the base paper and dry the ink;
[0038] The dried inner lining paper is printed with pearlescent pulp, and the pearlescent pulp is composed of the following components by weight: 500 parts of yellow powder, 13 parts of red powder, and 600 parts of alcohol; the viscosity requirements of the pearlescent pulp are: In the No. 4 viscosity cup filled with pearlescent pulp, the time required for the decanting of pearlescent pulp is 20s. The coating amount of pearl pulp on the inner liner paper is 1g / m 2 .
[0039] The parameters of the printing plate roller are: the number of lines of the color gravure plate roller is 160 circles, the cell is a regular hexagon, the cell opening is 60°, and the cell depth is 25-35μm. The angle...
Embodiment 2
[0043] The processing technology of aluminum-free lining paper for cigarettes includes the following steps:
[0044] The surface smoothness of the base paper is less than 200s, and the thinner coating is coated on the surface of the base paper, and the coating amount of the thinner coating is 2g / m 2 ;
[0045] Print yellow ink on the base paper and dry the ink;
[0046] The dried inner liner paper is printed with pearlescent pulp. The pearlescent pulp is composed of the following components by weight: 600 parts of yellow powder, 14 parts of red powder, and 550 parts of alcohol; the viscosity requirements of pearlescent pulp are: In the No. 4 viscosity cup filled with pearly pulp, the decanting time of pearly pulp is 21s. The coating amount of pearl pulp on the inner liner paper is 1g / m 2 .
[0047] The parameters of the printing plate roller are: the number of lines of the coloring gravure plate roller is 150 circles, the cell is a regular hexagon, the cell opening is 60°, and the ce...
Embodiment 3
[0050] The processing technology of aluminum-free lining paper for cigarettes includes the following steps:
[0051] The surface smoothness of the base paper is less than 200s, and the thinner coating is coated on the surface of the base paper. The coating amount of the thinner coating is 1.8g / m 2 ;
[0052] Print yellow ink on the base paper and dry the ink;
[0053] The dried inner liner paper is printed with pearlescent pulp. The pearlescent pulp is composed of the following components by weight: 700 parts of yellow powder, 15 parts of red powder, and 450 parts of alcohol; the viscosity of the pearlescent pulp is required to be: In the No. 4 viscosity cup filled with pearlescent pulp, the time required for the decanting of pearlescent pulp is 20s. The coating amount of pearl pulp on the inner liner paper is 1g / m 2 .
[0054] The parameters of the printing plate roller are: the number of lines of the coloring gravure plate roller is 150 circles, the cell is a regular hexagon, the c...
PUM
Property | Measurement | Unit |
---|---|---|
coating mass | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com