Environment-friendly shield tail sealing grease and preparation method thereof
A shield tail sealing and environment-friendly technology, applied in the petroleum industry, lubricating composition, etc., can solve the problems of poor sealing performance, large amount of sand layer, environmental pollution, etc., achieve good lubricity, good environmental protection performance, and simple preparation scheme Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0027] A preparation method of an environment-friendly shield tail sealing grease, the specific preparation steps of the preparation method of the environment-friendly shield tail sealing grease are as follows:
[0028] S1: Stir and mix the base oil, extreme pressure lithium base grease and viscosity improver: Weigh the base oil, extreme pressure lithium base grease and viscosity improver according to the mass specific gravity and put them in the kneader, turn on the kneader Stir and knead the internal raw materials, heat the inside of the kneader during the process of stirring and kneading, so that the temperature inside the kneader rises to 60-80 degrees Celsius, and make the kneader work for 2-3 hours to obtain a preliminary mixture;
[0029] S2: Add calcium carbonate powder to the mixed material after kneading, and continue mixing: add calcium carbonate powder to the preliminary mixed material obtained in step S1, start the kneader, continue to stir and mix for 10-12 minute...
Embodiment 1
[0034] Base oil, viscosity modifier, extreme pressure lithium grease, calcium carbonate powder and reinforcing fiber are as follows according to mass proportion: base oil 18Kg, viscosity modifier 26Kg, extreme pressure lithium grease 14Kg, calcium carbonate powder 6Kg and reinforcing fiber 14Kg.
[0035] The specific preparation steps of the preparation method of the environment-friendly shield tail sealing grease are as follows:
[0036] S1: Stir and mix the base oil, extreme pressure lithium base grease and viscosity improver: Weigh the base oil, extreme pressure lithium base grease and viscosity improver according to the mass specific gravity and put them in the kneader, turn on the kneader Stir and knead the internal raw materials, heat the inside of the kneader during the process of stirring and kneading, so that the temperature inside the kneader rises to 60 degrees Celsius, and make the kneader work for 2 hours to obtain a preliminary mixture;
[0037] S2: Add calcium c...
Embodiment 2
[0040] Base oil, viscosity improver, extreme pressure lithium base grease, calcium carbonate powder and reinforcing fiber are respectively according to mass proportion: base oil 20Kg, viscosity improver 28Kg, extreme pressure lithium base grease 16Kg, calcium carbonate powder 8Kg and reinforcing fiber 16Kg.
[0041] The specific preparation steps of the preparation method of the environment-friendly shield tail sealing grease are as follows:
[0042] S1: Stir and mix the base oil, extreme pressure lithium base grease and viscosity improver: Weigh the base oil, extreme pressure lithium base grease and viscosity improver according to the mass specific gravity and put them in the kneader, turn on the kneader Stir and knead the internal raw materials, heat the inside of the kneader during the process of stirring and kneading, so that the temperature inside the kneader rises to 70 degrees Celsius, and make the kneader work for 2.5 hours to obtain a preliminary mixture;
[0043] S2:...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com