Mixed flocculating agent and preparation method thereof
A flocculant and solution technology, which is applied in the field of mixed flocculant and its preparation, can solve the problems of high moisture content of sludge, long flocculation time, high turbidity, etc., and achieve the effects of reduced volume, good physical adsorption capacity, and increased sedimentation speed
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A mixed flocculant, comprising the following composition in parts by weight, 10 parts of sodium carboxymethylcellulose, 5 parts of polyacrylamide, 18 parts of chitosan, 7 parts of polyethyleneimine, 22 parts of caffeic acid, and 48 parts of clay And disodium hydrogen phosphate 6 parts.
[0020] A preparation method of a mixed flocculant, adding 1.8g of chitosan and 1g of sodium carboxymethyl cellulose to 200mL of water in turn, stirring evenly to obtain solution A, adding 0.5g of polyacrylamide, 0.7g of polyethyleneimine, Add 0.6 g of disodium hydrogen phosphate into solution A in sequence, stir evenly and cool to 25°C to obtain solution B, add 2.2 g of caffeic acid and 4.8 g of clay into solution B in sequence, stir with a magnetic stirrer for uniform reaction for 1 hour, put in 120 ℃ oven to obtain solid powder, which is the mixed flocculant.
Embodiment 2
[0022] A mixed flocculant, comprising the following composition in parts by weight, 5 parts of sodium carboxymethylcellulose, 5 parts of polyacrylamide, 8 parts of chitosan, 6 parts of polyethyleneimine, 20 parts of caffeic acid, and 48 parts of clay And disodium hydrogen phosphate 6 parts.
[0023] A preparation method of a mixed flocculant, adding 0.8g of chitosan and 0.5g of sodium carboxymethyl cellulose to 200mL of water in turn, stirring evenly to obtain solution A, mixing 0.5g of polyacrylamide and 0.6g of polyethyleneimine , disodium hydrogen phosphate 0.6g was added to solution A in turn, stirred evenly and then cooled to 20°C to obtain solution B, 2g caffeic acid and 4.8g clay were added to solution B in turn, stirred evenly with a magnetic stirrer for 1h, put in 100 °C in an oven to obtain a solid powder to obtain the mixed flocculant.
Embodiment 3
[0025] A mixed flocculant, comprising the following composition in parts by weight, 5 parts of sodium carboxymethylcellulose, 6 parts of polyacrylamide, 10 parts of chitosan, 6 parts of polyethyleneimine, 12 parts of caffeic acid, and 26 parts of clay And disodium hydrogen phosphate 6 parts.
[0026] A preparation method of a mixed flocculant, adding 1 g of chitosan and 0.5 g of sodium carboxymethyl cellulose to 200 mL of water in sequence, stirring evenly to obtain solution A, mixing 0.6 g of polyacrylamide, 0.6 g of polyethyleneimine, Add 0.6 g of disodium hydrogen phosphate into solution A in turn, stir evenly and cool to 20°C to obtain solution B, add 1.2 g of caffeic acid and 2.6 g of clay into solution B in turn, stir with a magnetic stirrer for 2 hours, put in 110 ℃ oven to obtain solid powder, which is the mixed flocculant.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com