A nematocyst and carrier technology, applied in the field of carrier for fixing jellyfish nematocysts and its preparation, can solve the problems that nematocysts are easy to drift out of the field of vision and easily irritate nematocysts, and achieve strong operability and equipment The effect of simple and fast preparation method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] 1) Weigh 5.0 g of gelatin particles and place them in a beaker, add 20 mL of distilled water, and cover the beaker with a glass petri dish to prevent water vapor from escaping during heating.
[0022] 2) Heat the beaker in a 70°C water bath.
[0023] 3) After the gelatin particles are melted, stir gently with a glass rod to mix the gelatin and water thoroughly and without bubbles in the gelatin. Use a pipette to add 1 mL of gelatin to the 12-well plate while it is hot. It is a carrier with a thickness of 0.3 cm. Such as figure 1 Shown.
Embodiment 2
[0025] 1) Weigh 5.0 g of gelatin particles and place them in a beaker, add 20 mL of distilled water, and cover the beaker with a glass petri dish to prevent water vapor from escaping during heating.
[0026] 2) Heat the beaker in a 70°C water bath.
[0027] 3) After the gelatin particles have melted, stir gently with a glass rod to mix the gelatin and water thoroughly and without bubbles in the gelatin. Use a pipette to add 1.5 mL of gelatin to the 12-well plate while it is hot. After cooling and solidification, It is a gelatin carrier with a thickness of 0.4 cm.
Embodiment 3
[0029] 1) Weigh 4.0 g of gelatin particles into a beaker, add 20 mL of distilled water, and cover the beaker with a glass petri dish to prevent water vapor from escaping during heating.
[0030] 2) Heat the beaker in a 70°C water bath.
[0031] 3) After the gelatin particles are melted, stir gently with a glass rod to mix the gelatin and water thoroughly and without bubbles in the gelatin. Use a pipette to add 1 mL of gelatin to the 12-well plate while it is hot. It is a gelatin carrier with a thickness of 0.3 cm.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com