Compounded oil field corrosion inhibitor and preparation method thereof
A corrosion inhibitor and oilfield technology, applied in the field of oilfield water treatment, can solve the problems of aggravated corrosion, failure of corrosion inhibitor, failure to slow down the corrosion of oil and water pipelines, etc., and achieves the effect of delaying corrosion rate, saving costs, and facilitating large-scale popularization and application.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0040] According to another aspect of the present invention, the present invention provides a kind of preparation method of compound type oil field corrosion inhibitor, comprises the following steps:
[0041] (1) Preparation of liquid A
[0042] Put a mixed solution of acetophenone and absolute ethanol into the first reaction kettle, add hydrochloric acid dropwise while stirring, adjust the pH value of the solution to 2, add formaldehyde and cyclohexylamine dropwise at 80°C, react under reflux for 10 hours, add Stir a small amount of absolute ethanol to obtain a reddish-brown liquid, then compound with potassium iodide and propynyl alcohol to obtain a Mannich corrosion inhibitor solution, then add fatty alcohol polyoxyethylene ether and fatty alcohol polyoxyethylene ether phosphate under normal temperature and pressure, Prepare liquid A. Among them, the Mannich corrosion inhibitor A solution is a Mannich acidification corrosion inhibitor of the aromatic ketone Mannich base se...
Embodiment 1
[0057] (1) Preparation of liquid A:
[0058] Add 160 mL of absolute ethanol into a five-neck glass flask, add 47 mL of acetophenone and stir evenly, slowly add hydrochloric acid solution dropwise, and adjust the pH value of the solution to 2. Add 68mL of formaldehyde and 47mL of cyclohexylamine dropwise at about 80°C at the same time using a constant pressure dropping funnel, reflux for 10 hours, add a small amount of absolute ethanol, and stir evenly. Add 36g of potassium iodide and 80mL of propynyl alcohol to compound A liquid.
[0059] (2) Preparation of liquid B:
[0060] 146 grams of oleic acid and 206 grams of diethylenetriamine were dropped into another five-necked glass flask and stirred evenly, and 39 g of xylene was added. Raise the temperature to 140-150°C and reflux for 4 hours. Heat up to 180°C to evaporate xylene, then continue to heat up to 250°C for 4 hours. After cooling down to 120°C, add 50g of formic acid and 50g of formaldehyde, stir evenly and add 56g...
Embodiment 2
[0063] Adopt the method identical with embodiment 1 to prepare A liquid and B liquid;
[0064] The A solution and the B solution were compounded according to the volume ratio of 1:1 to obtain the compound oilfield corrosion inhibitor II.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com