Formaldehyde removal air spray and preparation method thereof
An air spray and formaldehyde technology, which is applied in the field of formaldehyde removal air spray and its preparation, can solve the problems of weak adsorption capacity and poor formaldehyde removal effect, and achieve the effect of great use value
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] Step 1, weighing by weight percentage: honeysuckle extract 4%, peppermint extract 1%, clove extract 4%, perilla leaf extract 5%, sweet-scented osmanthus extract 5%, licorice extract 4%, trichosanthin water Extract 3%, activated carbon 7%, stable dispersant 1.5%, nano-silver 1%, composite nano-titanium dioxide (a mixture of 2% silicon compound nano-titanium dioxide, 1% iron compound nano-titanium dioxide and 1% zinc compound nano-titanium dioxide) 1.5%, the rest is deionized water;
[0030] Step 2, adding composite nano-titanium dioxide into deionized water, stirring evenly, and standing for 1.5 hours to obtain the first aqueous dispersion;
[0031] Step 3, adding the stable dispersant described in step 1 to the first aqueous dispersion obtained in step 2, standing for 2.5 hours, and stirring evenly to obtain a second aqueous dispersion;
[0032] Step 4, adding the remaining components described in step 1 except the stable dispersant, composite nano-titanium dioxide, an...
Embodiment 2
[0035] Step 1, weighing by weight percentage: honeysuckle extract 4%, peppermint extract 1%, clove extract 4%, perilla leaf extract 5%, sweet-scented osmanthus extract 5%, licorice extract 4%, trichosanthin water Extract 3%, activated carbon 7%, stable dispersant 1.5%, nano-silver 1%, composite nano-titanium dioxide (a mixture of 2% silicon compound nano-titanium dioxide, 1% iron compound nano-titanium dioxide and 1% zinc compound nano-titanium dioxide) 1.5%, the rest is deionized water;
[0036] Step 2, adding the composite nano-titanium dioxide into deionized water, stirring evenly, and standing for 1 hour to obtain the first aqueous dispersion;
[0037] Step 3, adding the stable dispersant described in step 1 to the first aqueous dispersion obtained in step 2, standing for 2 hours, and stirring evenly to obtain a second aqueous dispersion;
[0038] Step 4, adding the remaining components described in step 1 except the stable dispersant, composite nano-titanium dioxide, and...
Embodiment 3
[0041] Step 1, weighing by weight percentage: honeysuckle extract 4%, peppermint extract 1%, clove extract 4%, perilla leaf extract 5%, sweet-scented osmanthus extract 5%, licorice extract 4%, trichosanthin water Extract 3%, activated carbon 7%, stable dispersant 1.5%, nano-silver 1%, composite nano-titanium dioxide (a mixture of 2% silicon compound nano-titanium dioxide, 1% iron compound nano-titanium dioxide and 1% zinc compound nano-titanium dioxide) 1.5%, the rest is deionized water;
[0042] Step 2, adding composite nano-titanium dioxide into deionized water, stirring evenly, and standing for 2 hours to obtain the first aqueous dispersion;
[0043] Step 3, adding the stable dispersant described in step 1 to the first aqueous dispersion obtained in step 2, standing for 3 hours, and stirring evenly to obtain a second aqueous dispersion;
[0044]Step 4, adding the remaining components described in step 1 except the stable dispersant, composite nano-titanium dioxide, and dei...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com