A production method and brush technology, which can be applied to other ink pens, single-component polyamide artificial filaments, printing, etc., can solve the problems of inferior animal hair, poor elasticity of nylon hair, poor water retention rate, etc., and achieve good fiber properties and elasticity, prevent hair loss, and improve the service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A method for making a writing brush, comprising the following steps:
[0022] 1) heating and blending 10 parts by weight of nylon 6, 0.01 parts of rubber, and 0.5 parts of calcium carbonate, and then melting and processing them into modified nylon wool with a diameter of 0.05 mm;
[0023] 2) Soak rabbit hair, duck hair, and pig hair in soapy water for 50 minutes, then soak them in starch solution for 20 minutes, take them out and soak them in acetic acid for 3 minutes;
[0024] 3) Mix the processed rabbit hair, duck hair, pig hair and modified nylon hair with a carding machine according to the mass ratio of 1:1:0.5:0.5, and pick a part of the mixed pen core hair when making the pen core. Bundle, spread the bundle of hair on a flat plate, after grooming, and then roll up from one end to form a conical pen tip, install the tied pen tip on the pen tube, and add glue to connect.
Embodiment 2
[0026] A method for making a writing brush, comprising the following steps:
[0027] 1) heating and blending 15 parts by weight of nylon 6, 0.01 part of rubber, and 0.6 part of calcium carbonate, and then melting and processing it into modified nylon wool with a diameter of 0.1 mm;
[0028] 2) Soak rabbit hair, duck hair, and pig hair in soapy water for 75 minutes, then soak them in starch solution for 30 minutes, take them out and soak them in acetic acid for 5 minutes;
[0029] 3) Mix the treated rabbit hair, duck hair, pig hair and modified nylon hair with a carding machine according to the mass ratio of 1:1:1:1, and pick a part of the mixed pen core hair when making the pen core. Bundle, spread the bundle of hair on a flat plate, after grooming, and then roll up from one end to form a conical pen tip, install the tied pen tip on the pen tube, and add glue to connect.
Embodiment 3
[0031] A method for making a writing brush, comprising the following steps:
[0032] 1) 15 parts by weight of nylon 6, 0.02 parts of rubber, and 0.8 parts of calcium carbonate were heated and blended, then melted and processed into modified nylon wool with a diameter of 0.1 mm;
[0033] 2) Soak rabbit hair, duck hair, and pig hair in soapy water for 65 minutes, then soak them in starch solution for 30 minutes, take them out and soak them in acetic acid for 5 minutes;
[0034] 3) Mix the treated rabbit hair, duck hair, pig hair and modified nylon hair with a carding machine according to the mass ratio of 2:1:1:1, and pick a part of the mixed pen core hair when making the pen core. Bundle, spread the bundle of hair on a flat plate, after grooming, and then roll up from one end to form a conical pen tip, install the tied pen tip on the pen tube, and add glue to connect.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
concentration | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com