Temporary support device for high-voltage cable
A temporary support and high-voltage cable technology, which is applied in the direction of cable suspension, cable installation, electrical components, etc., can solve problems such as cable sagging and utility models are difficult to function, and achieve the effect of improving work efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0057] refer to Figure 1~2 , a temporary support device for high-voltage cables, comprising a base 1 and an anchoring mechanism 2 for installing and fixing the base 1, a left ear plate seat 3 is arranged on the left side of the upper part of the base 1, and a right ear is arranged on the upper right side of the base 1 Board seat 4, on the left ear plate seat 3 and the right ear plate seat 4, an inverted U-shaped connecting seat 5 is arranged, and a supporting rod body 6 is arranged on the connecting seat 5, and the upper end of the supporting rod body 6 is provided for clamping and A clamping mechanism that fixes high-voltage cables and has insulating properties. A pair of pull rings 7 are symmetrically arranged on the front and rear sides of the support rod body 6. The pull rings 7 are provided with pull ropes for pulling up and fixing the support rod body 6. 8. Fixed piles 9 for fixing the free ends of the pull ropes 8 are arranged symmetrically on the base 1 and on the fro...
Embodiment 2
[0082] The structure of the high-voltage cable temporary support device of this embodiment is basically the same as that of Embodiment 1, the difference is that:
[0083] The aluminum alloy is made of the following components in mass percentage:
[0084] Mg: 2.8%;
[0085] Si: 4.2%;
[0086] Mn: 0.28%;
[0087] Cr: 0.16%;
[0088] Zr: 0.23%;
[0089] Ti: 0.38%;
[0090] Yb: 0.25%;
[0091] The balance is Al and impurities with a content of ≤0.05%.
[0092] The preparation method of the aluminum alloy comprises the following steps:
[0093] Step S1: Carry out alloy smelting according to the above composition ratio, the alloy smelting temperature is 735°C, and keep warm for 10 minutes to obtain alloy melt 1;
[0094] Step S2: adding a refining agent to the obtained alloy melt 1 for refining, the refining temperature is 735° C., and the time is 12 minutes to obtain alloy melt 2;
[0095] Step S3: cooling and extruding the molten alloy 2 to obtain an ingot;
[0096] Step...
Embodiment 3
[0103] The structure of the high-voltage cable temporary support device of this embodiment is basically the same as that of Embodiment 1, the difference is that:
[0104] The aluminum alloy is made of the following components in mass percentage:
[0105] Mg: 2.2%;
[0106] Si: 3.6%;
[0107] Mn: 0.23%;
[0108] Cr: 0.12%;
[0109] Zr: 0.20%;
[0110] Ti: 0.36%;
[0111] Yb: 0.18%;
[0112] The balance is Al and impurities with a content of ≤0.05%.
[0113] The preparation method of the aluminum alloy comprises the following steps:
[0114] Step S1: Carry out alloy melting according to the above-mentioned composition ratio, the alloy melting temperature is 725°C, and keep warm for 12 minutes to obtain alloy melt 1;
[0115] Step S2: adding a refining agent to the obtained alloy melt 1 for refining, the refining temperature is 732° C., and the time is 15 minutes to obtain alloy melt 2;
[0116] Step S3: cooling and extruding the molten alloy 2 to obtain an ingot;
[0117...
PUM
Property | Measurement | Unit |
---|---|---|
Tensile strength | aaaaa | aaaaa |
Yield strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com