[0027] This embodiment provides a PVC conveyor belt waterproof layer, including a conveyor belt, the surface of the conveyor belt is provided with a waterproof layer, and the three components of the waterproof layer A, B, and C are compounded according to the ratio of A: B: C = 2: 2: 1. C comprises the following components in parts by mass:
[0028] Component A includes the following components in parts by mass: Type 5 PVC: 35 parts, water glass: 9 parts, dispersant: 9 parts, graphite powder: 16 parts, potassium hydrogen phthalate: 3 parts, nano Silicon dioxide: 13 parts, benzyl alcohol: 13 parts;
[0029] Component B includes the following components in parts by mass: propylene carbonate: 11 parts, PVC foam regulator LP-40: 5 parts, 3-butanediol: 9 parts, 3-methylphenol: 12 parts Parts, plasticizer: 8 parts, C5 hydrogenated petroleum resin: 7 parts, antioxidant: 6 parts;
[0030] Component C includes the following components in parts by mass: dimethylethanolamine: 9 parts, ...
Embodiment 2
[0039] This embodiment provides a PVC conveyor belt waterproof layer, including a conveyor belt, the surface of the conveyor belt is provided with a waterproof layer, and the three components of the waterproof layer A, B, and C are compounded according to the ratio of A: B: C = 2: 2: 1. C comprises the following components in parts by mass:
[0040] Component A includes the following components in parts by mass: Type 5 PVC: 40 parts, water glass: 12 parts, dispersant: 11 parts, graphite powder: 20 parts, potassium hydrogen phthalate: 7 parts, nano Silicon dioxide: 16 parts, benzyl alcohol: 22 parts;
[0041] Component B includes the following components in parts by mass: propylene carbonate: 16 parts, PVC foam regulator LP-40: 10 parts, 3-butanediol: 14 parts, 3-methylphenol: 17 parts Parts, plasticizer: 14 parts, C5 hydrogenated petroleum resin: 11 parts, antioxidant: 8 parts;
[0042] Component C includes the following components in parts by mass: dimethylethanolamine: 14 ...
Embodiment 3
[0051] This embodiment provides a PVC conveyor belt waterproof layer, including a conveyor belt, the surface of the conveyor belt is provided with a waterproof layer, and the three components of the waterproof layer A, B, and C are compounded according to the ratio of A: B: C = 2: 2: 1. C comprises the following components in parts by mass:
[0052] Component A includes the following components in parts by mass: Type 5 PVC: 38 parts, water glass: 11 parts, dispersant: 10 parts, graphite powder: 18 parts, potassium hydrogen phthalate: 5 parts, nano Silicon dioxide: 14 parts, benzyl alcohol: 18 parts;
[0053] Component B includes the following components in parts by mass: propylene carbonate: 14 parts, PVC foam regulator LP-40: 8 parts, 3-butanediol: 12 parts, 3-methylphenol: 15 parts Parts, plasticizer: 10 parts, C5 hydrogenated petroleum resin: 8 parts, antioxidant: 7 parts;
[0054] Component C includes the following components in parts by mass: dimethylethanolamine: 11 pa...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com