Production method of light micro-foamed molded protective barrel product
A production method and technology of protective cylinders, applied in the direction of adhesives, etc., to achieve the effect of improved antistatic performance, excellent antistatic performance, and little decrease in mechanical performance strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0044] (1) Preparation of antistatic raw materials.
[0045] (2) The preparation of antistatic raw materials is carried out according to the following process:
[0046] The main raw material specifications and manufacturers used in the preparation of antistatic materials are shown in Table 1.
[0047] Table 1 Raw Material Specifications and Manufacturers
[0048]
[0049] (2.1) Extrusion granulation process: Weigh 17.88kg of PA66 resin, 0.6kg of antistatic agent P18, 0.2kg of carbon black, 0.2kg of graphite, and 0.1kg of polytetrafluoroethylene. Antioxidant 20g, toughening agent 1kg; add to the high-speed mixer and mix, first stir at low speed for 10s, then stir at high speed for 20s, release it into the prepared bag, transfer to the twin-screw extruder to extrude and granulate, extrude The process parameters are shown in Table 2.
[0050] Table 2 Extrusion process of antistatic nylon 66 material
[0051]
[0052] Note: The extruder is not limited to the model, the sam...
Embodiment 2
[0067] (1) The preparation of the antistatic raw material is the same as in Example 1.
[0068] (2) The preparation process of the antistatic raw material is the same as in Example 1.
[0069] (2.1) The extrusion granulation process is the same as that in Example 1.
[0070] (2.2) Injection molding process: The raw materials produced through the (2.1) process need to be dried in an oven first, the thickness of the material layer is 2cm, the temperature of the baking material is 120°C, and the drying time is 5h, and then the micro-foaming injection machine Molded into products. The micro-foaming injection molding process is shown in Table 5;
[0071] Table 5 Protection cylinder micro-foam molding process
[0072]
[0073]
[0074] (2.3) The flocking process is the same as in Example 1.
[0075] Product qualification testing is the same as in Example 1.
[0076] (1) The detection method of the wear resistance of the flocking layer is the same as that in Example 1.
...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com