Producing method of wallpaper
A production method and wallpaper technology, which is applied in the field of decorative materials, can solve the problems of insufficient foaming height, difficult control, and thickness, and achieve the effect of not easy to fall off and firmly bonded
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A method for producing wallpaper, comprising the steps of:
[0017] Step 1: Unwind the non-woven paper on the printing machine, and then send it to the coating machine;
[0018] Step 2: The coating machine uses the first PVC foam slurry to coat the surface of the non-woven paper with a PVC layer. The coating temperature is 170°C. After plasticizing, it is foamed and cooled at 210°C to obtain a foamed semi-finished product. ;
[0019] Step 3: Unwind the foamed semi-finished product and send it to the rotary screen printing device. The rotary screen printing device uses the second PVC foaming slurry to print the color and three-dimensional simulation pattern on the surface layer of the foamed semi-finished product, and pass through 170 ° C Hot air drying, and then cooling to get printed semi-finished products;
[0020] Step 4: Send the printed semi-finished product into the oven to heat up for correlative matching and foaming. The heating and foaming temperature is 200°...
Embodiment 2
[0026] A method for producing wallpaper, comprising the steps of:
[0027] Step 1: Unwind the non-woven paper on the printing machine, and then send it to the coating machine;
[0028] Step 2: The coating machine uses the first PVC foaming slurry to coat the surface of the non-woven paper with a PVC layer. The coating temperature is 180°C. After plasticizing, it is foamed and cooled at 220°C to obtain a foamed semi-finished product. ;
[0029] Step 3: Unwind the foamed semi-finished product and send it to the rotary screen printing device. The rotary screen printing device uses the second PVC foaming slurry to print the color and three-dimensional simulation pattern on the surface layer of the foamed semi-finished product, and pass through 175 ° C Hot air drying, and then cooling to get printed semi-finished products;
[0030] Step 4: Put the printed semi-finished product into the oven to heat up for correlative matching and foaming. The heating and foaming temperature is 17...
Embodiment 3
[0036] A method for producing wallpaper, comprising the steps of:
[0037] Step 1: Unwind the non-woven paper on the printing machine, and then send it to the coating machine;
[0038] Step 2: The coating machine uses the first PVC foaming slurry to coat the surface of the non-woven paper with a PVC layer. The coating temperature is 175°C. After plasticizing, it is foamed and cooled at 210°C to obtain a foamed semi-finished product. ;
[0039] Step 3: Unwind the foamed semi-finished product and send it to the rotary screen printing device. The rotary screen printing device uses the second PVC foaming slurry to print the color and three-dimensional simulation pattern on the surface layer of the foamed semi-finished product, and pass through 180°C Hot air drying, and then cooling to get printed semi-finished products;
[0040] Step 4: Send the printed semi-finished product into the oven to heat up for correlative matching and foaming. The heating and foaming temperature is 190...
PUM
Property | Measurement | Unit |
---|---|---|
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com