Children water-writing interior wall paint capable of turning transparent while contacting water
A water-contacting, transparent technology, applied in coatings, latex paints, etc., can solve the problem of young children not being able to control themselves well, and achieve the effect of reducing cleaning trouble and easy to use.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018]
[0019] The preparation method is as follows: add water, dispersant, wetting agent and modifier into the container, stir with a mixer at a low speed (about 500 rpm) for about 10 minutes, slowly add the mixture of kaolin and molecular sieve, and raise the mixer The speed of rotation (about 1500 rpm) lasts for about 30 minutes, then reduce the speed of the mixer to 300--400 rpm. Slowly add emulsion, film-forming aids, and leveling agents, and disperse for 15-20 minutes. Slowly add the thickener dropwise before the end of stirring.
Embodiment 2
[0021]
[0022] The preparation method is as follows: add water, dispersant, wetting agent and modifier into the container, stir with a mixer at a low speed (about 500 rpm) for about 10 minutes, slowly add the mixture of kaolin and molecular sieve, and raise the mixer The speed of rotation (about 1500 rpm) lasts for about 30 minutes, then reduce the speed of the mixer to 300--400 rpm. Slowly add emulsion, film-forming aids, and leveling agents, and disperse for 15-20 minutes. Slowly add the thickener dropwise before the end of stirring.
Embodiment 3
[0024]
[0025] The preparation method is as follows: add water, dispersant, wetting agent and modifier into the container, stir with a mixer at a low speed (about 500 rpm) for about 10 minutes, slowly add the mixture of kaolin and molecular sieve, and raise the mixer The speed of rotation (about 1500 rpm) lasts for about 30 minutes, then reduce the speed of the mixer to 300--400 rpm. Slowly add emulsion, film-forming aids, and leveling agents, and disperse for 15-20 minutes. Slowly add the thickener dropwise before the end of stirring.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com