[0009] (1) Take a closed reactor and set the temperature of the reactor to 70°C; (2) Open the closed reactor and add 210kg of water, 55kg of ethanol, 4kg of ammonium dihydrogen phosphate, hydrogen phosphate Calcium is 3kg, carboxymethylcellulose sodium is 9kg, stir with a mixer at a stirring speed of 200r / min; (3) After stirring evenly, add ethoxyaminopropyl polydimethylsiloxane to the reaction kettle 4kg for mannan, 6kg for mannan, and 3kg for octylphenol polyoxyethylene ether, stir with a mixer at a stirring speed of 150r / min, and stir evenly; (4) Put the evenly stirred finishing agent into a storage bucket, Sealed after being filled with nitrogen.
Embodiment 2
[0011] (1) Take a closed reactor and set the temperature of the reactor to 66°C; (2) Open the closed reactor and add 215kg of water, 35kg of ethanol, 3kg of ammonium dihydrogen phosphate, hydrogen phosphate Calcium is 5kg, sodium carboxymethyl cellulose is 7kg, stir with a mixer, and the stirring speed is 200r / min; (3) After stirring evenly, add ethoxyaminopropyl polydimethylsiloxane to the reaction kettle 5kg for mannan, 5kg for mannan, and 4kg for octylphenol polyoxyethylene ether, stir with a mixer at a stirring speed of 150r / min, and stir evenly; (4) Put the evenly stirred finishing agent into a storage bucket, Sealed after being filled with nitrogen.
Embodiment 3
[0013] (1) Take a closed reactor and set the temperature of the reactor to 68°C; (2) Open the closed reactor and add 220kg of water, 45kg of ethanol, 2kg of ammonium dihydrogen phosphate, hydrogen phosphate Calcium is 4kg, sodium carboxymethyl cellulose is 8kg, stir with a mixer, and the stirring speed is 200r / min; (3) After stirring evenly, add ethoxyaminopropyl polydimethylsiloxane to the reaction kettle 6kg for mannan, 6kg for mannan, and 5kg for octylphenol polyoxyethylene ether, stir with a mixer at a stirring speed of 150r / min, and stir evenly; (4) Put the evenly stirred finishing agent into a storage bucket, Sealed after being filled with nitrogen.
[0014] Soak the cotton suit in the finishing agent of Example 1, Example 2, and Example 3 at room temperature for 1 hour. After soaking and rolling, the excess rate is 65%, and it is dried at 95°C. The test standards for water repellency and oil repellency are AATCC22-2010 and AATCC118, and the results are shown in the tab...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com