A technology for reorganizing decoration and manufacturing methods, applied in chemical instruments and methods, flat products, lamination devices, etc., can solve problems such as not suitable for wire drawing processing, achieve good chemical stability, reduce brittleness, and reduce production costs.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A method for manufacturing an antique brushed recombined decorative veneer, the method includes the following steps:
[0029] 1. Cut the restructured decorative material into 0.5mm restructured decorative veneer;
[0030] 2. Use a modified urea-formaldehyde resin adhesive to paste a non-woven hot-melt adhesive interlining on the back of the restructured decorative veneer, and the thickness of the interlining is 0.06mm. The hot pressing temperature is 95°C, the pressure is 0.8Mpa, and the time is: 80 seconds;
[0031] 3. Improve the wire brush structure of the drawing roller so that the pitch of the soft and hard steel wires is 15mm;
[0032] 4. Use 3mm plywood as the conveying lining board, and glue the two ends of the restructured decorative veneer to the two ends of the conveying lining board; in order to facilitate separation after drawing, use double-sided tape for bonding;
[0033] 5. Continuously, drawing the recombined decorative veneer one by one;
[0034] 6....
Embodiment 2
[0037] A method for manufacturing an antique brushed recombined decorative veneer, the method includes the following steps:
[0038] 1. Cut the restructured decorative material into 0.5mm restructured decorative veneer;
[0039] 2. Use modified urea white latex adhesive to paste kraft paper on the back of the restructured decorative veneer, and the thickness of the interlining cloth is 0.08mm. The hot pressing temperature is 100°C, the pressure is 1.0Mpa, and the time is: 90 seconds;
[0040] 3. Improve the wire brush structure of the drawing roller so that the pitch of the soft and hard steel wires is 25mm;
[0041] 4. Use 3mm plywood as the conveying liner, and glue the two ends of the restructured decorative veneer to the two ends of the conveying liner; in order to facilitate separation after drawing, use transparent tape to bond;
[0042] 5. Continuously, drawing the recombined decorative veneer one by one;
[0043] 6. Perform post-processing such as surface sanding, e...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com