Potassium-chloride product and preparation method thereof
A technology of potassium chloride and its products, which is applied in the field of potassium chloride products and its preparation, and can solve the problems that potassium chloride does not increase the average particle size of potassium chloride crystal particles, and the purity is low.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0047] A. Dissolve edible potassium chloride in water to form a saturated solution, evaporate and concentrate at 105°C for a period of time, and then add potassium chloride seed crystals with a crystal size of 0.6mm in proportion to 100% of the potassium chloride mass in the saturated solution , Forming a thick slurry;
[0048] B. Place the concentrated slurry obtained in step A in an ordinary crystallization tank to cool to 35°C for crystallization for 5 hours, and then separate and dry the crystals obtained in the crystallization tank to obtain the potassium chloride product, Example 1.
Embodiment 2
[0050] A. Dissolve food grade potassium chloride in water to form a saturated solution, evaporate and concentrate at 100°C for a period of time, and then add potassium chloride seed crystals with a crystal size of 0.6mm in proportion to 100% of the potassium chloride mass in the saturated solution , Forming a thick slurry;
[0051] B. Place the concentrated slurry obtained in step A in an ordinary crystallization tank to cool to 35°C for crystallization for 60 minutes, and then separate and dry the crystals obtained in the crystallization tank to obtain the potassium chloride product, Example 2.
Embodiment 3
[0053] A. Dissolve edible potassium chloride in water to form a saturated solution, evaporate and concentrate at 100°C for a period of time, and then add potassium chloride seed crystals with a crystal size of 0.5 mm in proportion to 60% of the potassium chloride mass in the saturated solution , Forming a thick slurry;
[0054] B. Place the concentrated slurry obtained in step A in an ordinary crystallization tank to cool to 30°C for crystallization for 30 minutes, and then separate and dry the crystals obtained in the crystallization tank to obtain the potassium chloride product (Example 3).
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com