[0034] Example 1 Injection molding method of environmental protection, energy saving and degradable disposable vaginal dilator:
[0035] Using the degradable base material of formula 1, its injection molding method is:
[0036] The first step, vacuum drying: the degradable substrate pellets of Formula 1 were vacuum-dried at 50° C. for 4 hours, and then used.
[0037] The second step, injection molding: Add the dried degradable substrate pellets of Formula 1 to the injection molding machine for injection molding. The barrel temperature is set as: feed inlet 160°C, compression section 165°C, metering section 170°C , nozzle 170°C;
[0038] Mold temperature: 25°C;
[0039] The injection pressure is: the first section is 75pa, the second section is 80Mpa, and the third section is 50Mpa;
[0040] Injection time: 4 seconds;
[0041] The holding time is: 0 seconds;
[0042] The screw speed is: 180 rpm.
[0043] The upper expansion sheet (1) and the lower expansion sheet (2) of t...
Embodiment 2
[0044]Example 2 Injection molding method of environmental protection, energy saving and degradable disposable vaginal dilator:
[0045] Using the degradable base material of formula 2, its injection molding method is:
[0046] The first step, vacuum drying: the degradable substrate pellets of Formula 2 were vacuum-dried at 55° C. for 3 hours, and then used.
[0047] The second step, injection molding: add the dried degradable substrate pellets of formula 2 to an injection molding machine for injection molding.
[0048] The barrel temperature is set as: feed inlet 155°C, compression section 160°C, metering section 165°C, nozzle 155°C;
[0049] Mold temperature: 30°C;
[0050] The injection pressure is: the first section is 65pa, the second section is 70Mpa, and the third section is 50Mpa;
[0051] Injection time: 5 seconds;
[0052] The holding time is: 0 seconds;
[0053] The screw speed is: 180 rpm.
[0054] The upper expansion sheet (1) and the lower expansion sheet (2...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com