Method for rapidly synthesizing nanometer 3A molecular sieve
A molecular sieve and nano-technology, which is applied in the field of rapid synthesis of nano-3A molecular sieves, can solve the problems of high process cost, high-temperature calcination, and large energy loss, and achieve the effects of simple reaction procedures, high product purity, and low price
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0026] Weigh 40.0g sodium hydroxide, 16.8g potassium hydroxide and 138.6g potassium silicate respectively, mix the three and dissolve them in 270ml water, then weigh 70.2g aluminum hydroxide and add to the mixture and stir until it is fully After dissolving, heat to 95°C in the reaction kettle for constant temperature crystallization, weigh 62.4g of aluminum hydroxide and 42.0g of amorphous silicon dioxide at the same time, add them to the mixed solution evenly for 0.5-1h under stirring, and Constant temperature crystallization at 95°C for 2 hours, the crystallized product was filtered and dried to obtain a nanometer 3A molecular sieve product with an average particle size of 120nm.
example 2
[0028] Weigh 40.0g sodium hydroxide, 22.4g potassium hydroxide and 154.0g potassium silicate respectively, mix the three and dissolve them in 390ml water, then weigh 78.0g aluminum hydroxide and add to the mixed solution and stir until fully After dissolving, heat to 90°C in the reaction kettle for constant temperature crystallization, weigh 61.6g of aluminum hydroxide and 39.5g of amorphous silicon dioxide at the same time, add them to the mixed solution evenly for 0.5-1h under stirring, and Constant temperature crystallization at 90°C for 2.5 hours, the crystallized product was filtered and dried to obtain a nanometer 3A molecular sieve product with an average particle size of 190nm.
example 3
[0030] Weigh 40.0g of sodium hydroxide, 22.4g of potassium hydroxide and 169.4g of potassium silicate respectively, mix the three and dissolve them in 330ml of water, then weigh 85.8g of aluminum hydroxide and add to the mixture and stir until fully After dissolving, heat to 87°C in the reaction kettle for constant temperature crystallization, weigh 54.6g of aluminum hydroxide and 36.0g of amorphous silicon dioxide at the same time, add them to the mixed solution evenly for 0.5~1h under stirring, and Constant temperature crystallization at 87°C for 3.0 hours, the crystallized product was filtered and dried to obtain a nanometer 3A molecular sieve product with an average particle size of 280nm.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com