Embodiment 1
[0024] The method of making ink weighing up to 1,000 grams mainly includes processes such as refining smoke, mixing glue, pounding with a pestle, forming, baking, setting the shape, and drying the ink. The production method is as follows:
[0025] (1) Selection of materials for making ink sets: choose ten dragon tree wood for making ink sets, first store it on the first floor for one year, then move it to the second floor for one year, and then store it in a place with a higher temperature on the third floor for another year more than a year. It is then carved into an ink mold.
[0026] (2) Tobacco refining: the powdery material extracted by incompletely burning pine trees with a cigarette lighter is tobacco material; the obtained tobacco material is first rinsed, and impurities are removed with a 40-mesh sieve.
[0027] (3) Mixing glue: Mix the smoke material and rubber material in a ratio of 1:1.1, and stir it with a mixer with a power of 5000W and a speed of 300 rpm for 6 ...
Embodiment 2
[0033] Here's how to make a large ink weighing up to 5000 grams:
[0034] (1) Selection of materials for making ink sets: choose ten dragon tree wood for making ink sets, first store it on the first floor for one year, then move it to the second floor for one year, and then store it in a place with a higher temperature on the third floor for another year more than a year. It is then carved into an ink mold.
[0035] (2) Tobacco refinement: the powdery substance extracted by the method of incompletely burning Huangshan pine with a cigarette lighter is the tobacco material; the obtained tobacco material is first rinsed, and impurities are removed with a 40-mesh sieve.
[0036] (3) Mixing glue: Mix the smoke material and rubber material in a ratio of 1:1.2, and stir it with a mixer with a power of 5000W and a speed of 300 rpm for 7 minutes. When stirring, it will generate temperature by itself to make the ink embryo more transparent. It is more viscous. After stirring evenly, t...
Embodiment 3
[0042] The method of making a large ink weighing up to 20,000 grams is as follows:
[0043] (1) Selection of materials for making ink sets: choose ten dragon tree wood for making ink sets, first store it on the first floor for one year, then move it to the second floor for one year, and then store it in a place with a higher temperature on the third floor for another year more than a year. It is then carved into an ink mold.
[0044] (2) Tobacco refinement: the powdery substance extracted by the method of incompletely burning Huangshan pine with a cigarette lighter is the tobacco material; the obtained tobacco material is first rinsed, and impurities are removed with a 40-mesh sieve.
[0045] (3) Mixing glue: Mix the smoke material and the rubber material in a ratio of 1:1.4, and stir it with a mixer with a power of 5000W and a speed of 300 rpm for 8 minutes. When stirring, it will generate temperature by itself to make the ink embryo more transparent. It is more viscous. Af...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com