[0013] The initial conditions of wastewater are: total cyanide concentration, 3200mg / L; pH value, 10.5; copper ion concentration, 1800mg / L. The operation method is as follows: take 1000 mL of the waste water, add 1 g of elemental aluminum powder, fully stir the waste water and the aluminum powder, react for 2 hours, and perform centrifugation. The content of copper ions in the supernatant was measured to be 212mg / L, and the removal rate of copper ions was 88.2%.
Embodiment 2
[0015] The initial conditions of wastewater are: total cyanide concentration, 3800mg / L; pH value, 10.0; copper ion concentration, 2100mg / L. The operation method is as follows: take 1000mL of the waste water, add 2g of elemental aluminum flakes, stir the waste water for 2.5 hours, transfer the waste water to another beaker, add 2mL of coagulant for coagulation and precipitation for 30 minutes. The content of copper ions in the supernatant was measured to be 393mg / L, and the removal rate of copper ions was 81.3%. The coagulant is polyaluminum chloride with a concentration of 10g / L.
Embodiment 3
[0017] The initial conditions of wastewater are: total cyanide concentration, 3500mg / L; pH value, 11.5; copper ion concentration, 2050mg / L. The operation method is as follows: take 1000 mL of the waste water, add 2 g of elemental phosphorus powder, fully stir the waste water and phosphorus powder, react for 3 hours, and filter and separate. The content of copper ions in the filtrate was measured to be 228 mg / L, and the removal rate of copper ions was 88.9%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com