Liquid foundation added with pearl powder
A pearl powder and liquid foundation technology, applied in the directions of body powder, cosmetic preparations, dressing preparations, etc., can solve the problems of absorption, affect the absorption rate of active ingredients, affect the beauty effect, etc., and achieve the effect of lightening pigment and inhibiting melanin. Create and remove makeup easily
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Take 4kg of polydimethylsiloxane, 1kg of cetearyl alcohol, 4kg of isononyl isononanoate, 5kg of glycerin, 3kg of pearl powder, 3kg of isopropyl palmitate, 4kg of butylene glycol, dimer glycol Carbonate 1kg, acetylcysteine / collagen amino acid 1kg, cetearyl alcohol / coco glucoside 2kg, acrylic acid (ester) / C10-30 alkanol acrylate crosspolymer 0.1kg, triethanolamine 0.1kg, 0.3kg of phenoxyethanol, 0.4kg of ferric oxide, 71.4kg of deionized water.
[0015] Soak acrylic acid (ester) / C10-30 alkanol acrylate cross-linked polymer in deionized water for 2 hours, then put it into the emulsification pot, put glycerin, pearl powder, butanediol into the emulsification pot and heat to 80°C, stir well , keep warm for 20 minutes; dimethicone, cetearyl alcohol, isononyl isononanoate, isopropyl palmitate, dimer glycol carbonate, cetearyl alcohol / coconut oil Add glucoside, ferric oxide, and phenoxyethanol into the oil pan and heat to 80°C and stir evenly; pump the raw materials in the oil...
Embodiment 2
[0017] According to the formula, take polydimethylsiloxane 10kg, cetearyl alcohol 6kg, isononyl isononanoate 12kg, glycerin 16kg, pearl powder 10kg, isopropyl palmitate 10kg, butylene glycol 12kg, dimer Body glycol carbonate 6kg, acetylcysteine / collagen amino acid 8kg, cetearyl alcohol / cocoyl glucoside 6kg, acrylic acid (ester) / C10-30 alkanol acrylate crosspolymer 0.6kg , 0.6kg of triethanolamine, 1.0kg of phenoxyethanol, 0.4kg of ferric oxide, and 101.4kg of deionized water.
[0018] Soak acrylic acid (ester) / C10-30 alkanol acrylate cross-linked polymer in deionized water for 3 hours, then put it into the emulsification pot, put glycerin, pearl powder, butanediol into the emulsification pot, heat to 85°C, stir well , keep warm for 30 minutes; dimethicone, cetearyl alcohol, isononyl isononanoate, isopropyl palmitate, dimer glycol carbonate, cetearyl alcohol / coconut oil Add glucoside, ferric oxide, and phenoxyethanol into the oil pan and heat to 80°C and stir evenly; pump the ...
Embodiment 3
[0020] According to the formula, take 10kg of polydimethylsiloxane, 4kg of cetearyl alcohol, 10kg of isononyl isononanoate, 12kg of glycerin, 8kg of pearl powder, 8kg of isopropyl palmitate, 10kg of butylene glycol, dimer Body glycol carbonate 4kg, acetylcysteine / collagen amino acid 4kg, cetearyl alcohol / coco glucoside 5kg, acrylic acid (ester) / C10-30 alkanol acrylate crosspolymer 0.3kg , 0.3kg of triethanolamine, 0.8kg of phenoxyethanol, 0.4kg of ferric oxide, and 123.2kg of deionized water.
[0021] Soak acrylic acid (ester) / C10-30 alkanol acrylate crosslinked polymer in deionized water for 4 hours and put it into the emulsification pot, put glycerin, pearl powder and butanediol into the emulsification pot and heat to 82°C, stir evenly , keep warm for 30 minutes; dimethicone, cetearyl alcohol, isononyl isononanoate, isopropyl palmitate, dimer glycol carbonate, cetearyl alcohol / coconut oil Add glucoside, ferric oxide, and phenoxyethanol into the oil pan and heat to 80°C and ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com