Cementing material, preparation and use thereof
A technology of cementing material and petroleum resin, applied in the field of cementing material, can solve the problems of polluting the environment, unfavorable promotion and use, peeling and the like
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1~5
[0026] Raw materials used:
[0027] Aromatic oil, produced by Taiwan CNPC Co., Ltd., trade name: Guoguang brand rubber softening oil, viscosity at 40°C: 3.1Pa.S, flash point: 253°C, aromatic content: 74.7wt%, density at 15°C: 0.94g / cm3 .
[0028] B C9 petroleum resin, Korea Kolon company product, trade name: Hikotack P140, softening point 145 ℃, average molecular weight (GPC method) 2200
[0029] C N, N'—Ethylene bisoleic acid amide, produced by Jiangxi Weike Oleochemical Co., Ltd.
[0030] D SIS, produced by Kraton, trade name: D-1107.
[0031] Heat the aromatic oil to 175°C, then add C9 petroleum resin, N,N'-ethylene bisoleic acid amide and SIS, and stir with a stirrer at a speed of 200 rpm for 60 minutes to prepare the finished cement material. The specific composition ratio (percentage by weight) and the results of the cementitious material detected by the detection method specified in the standard JTJ052-2000 of the Ministry of Communications Standard "Testing Procedu...
PUM
Property | Measurement | Unit |
---|---|---|
Viscosity | aaaaa | aaaaa |
Flash point | aaaaa | aaaaa |
Density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com