Drying agent for absorbing ammonia
A desiccant and ammonia technology, applied in inorganic chemistry, animal husbandry, other chemical processes, etc., can solve the problems of unfavorable animal growth, humid environment, etc., achieve the effect of long action time, reduce humidity, and improve breeding benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0038] Get 40g of phosphate rock and pulverize it, mix it evenly with 40g of zeolite powder, add 100ml of sulfuric acid to react, after fully aging, filter out the filter cake, dry and pulverize it, and dry at 120°C for 4 hours to obtain 40g of zeolite powder, 33g of Ca(H 2 PO 4 ) 2 and 11gCaSO 4 2H 2 A mixture of O; take nano-kaolin 13g and CuSO 4 1.98g, FeSO 4 1 g was mixed evenly, and dried at 100°C for 1 hour to obtain a mixed powder; all the powders prepared above were mixed, and 0.02 g of mugwort oil was added according to the above weight portion, and then mixed evenly to obtain the desired desiccant.
Embodiment 2
[0040] After taking 42g of phosphate rock and pulverizing it, mix it with 30g of zeolite powder evenly, add 100ml of sulfuric acid to react, after fully ripening, filter out the filter cake, dry and pulverize, and dry at 120°C for 4 hours to obtain 30g of zeolite powder, 35g of Ca(H 2 PO 4 ) 2 and 10gCaSO 4 2H 2 The mixture of O; take nano-kaolin 25g and CuSO 4 0.5g, FeSO 4 2g was mixed evenly, and dried at 100°C for 1 hour to obtain a mixed powder; all the powders prepared above were mixed, and 0.05g of mugwort oil was added according to the above weight portion, and then mixed evenly to obtain the desired desiccant.
Embodiment 3
[0042] After taking 48g of phosphate rock and pulverizing it, mix it with 38g of zeolite powder evenly, add 100ml of sulfuric acid to react, after fully ripening, filter out the filter cake, dry and pulverize, and dry at 120°C for 4 hours to obtain 38g of zeolite powder, 25g of Ca(H 2 PO 4 ) 2 and 20gCaSO 4 2H 2 A mixture of O; take nano-kaolin 10g and CuSO 4 2g, FeSO 4 Mix 1.3g evenly, dry at 100°C for 1 hour to get the mixed powder; mix all the powders prepared above, add 0.01g mugwort oil according to the above weight parts, and mix evenly to get the desired desiccant .
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com