Potassium leach-out exploitation method from mamanite ore
A mining method and polyhalite technology, which are applied in the direction of improving process efficiency, can solve the problems of inability to achieve operating conditions and have not been developed and utilized, and achieve satisfactory development and utilization effects, wide applicability, and simple solution leaching mining methods. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] In this example, the simulation experiment was carried out with Nongle polyhalite in Quxian County, Sichuan Province, and the K content in the ore was 14.8%. with 5% CaCl 2 Solution 2500ml is leaching and leaching 250g polyhalite, the ore particle size is 2mm, the percolation speed is 0.75m / d, the percolation column is Φ25mm×h400mm (the height of the sample is 300mm), and the obtained leachate is 2300ml, of which K + Concentration of 13.45g / l,, K + The leaching rate was 82.5%.
Embodiment 2
[0026] In this example, the simulation experiment is still carried out with Nongle polyhalite in Quxian County, Sichuan Province, and the K content in the ore is 15.15%. with 5% CaCl 2 150g of polyhalite was obtained by leaching and leaching of solution 1600ml, the particle size of the ore sample was 5mm, the percolation velocity was 0.55m / d, the percolation column was Φ25mm×h400mm (the height of the sample was 250mm), and the obtained leachate was 1420ml, of which K + Concentration of 13.05g / l,, K + The leaching rate is 81.55%.
Embodiment 3
[0028] In this example, the polyhalite in Dawenkou, Shandong Province was used for the simulation experiment, and the K content in the ore was 10.8%. with 5% CaCl 2 Solution 2000ml is leached to extract 200g polyhalite, the ore particle size is 2mm, the percolation speed is 0.75m / d, the percolation column is Φ25mm×h400mm (the height of the sample is 300mm), and the obtained leachate is 1850ml, of which K + Concentration of 9.45g / l,, K + The leaching rate was 80.9%.
[0029] Example 3
[0030] In this example, the polyhalite in Dawenkou, Shandong Province was used for the simulation experiment, and the K content in the ore was 10.8%. with 5% CaCl 2 2500ml of the solution is leached to extract 200g of polyhalite, the ore particle size is 8mm, the percolation speed is 0.5m / d, the percolation column is Φ25mm×h400mm (the height of the sample is 300mm), and the obtained leachate is 2250ml, of which K + Concentration of 6.45g / l,, K + The leaching rate was 74.7%.
[0031] The p...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com