A water-retaining agent and multi-component technology, which is applied in the field of multi-component low-cost water-retaining agent and its preparation, can solve the problems that are not conducive to large-scale continuous production, serious production environment pollution, and production cost reduction, and achieve large-scale production Production, good gel strength, long-term effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] Example 1. First add 38.5% acrylamide aqueous solution and 1% N,N'-methylenebisacrylamide aqueous solution to the mixer at a ratio of 1:0.01, and adjust with sodium hydroxide under stirring. Polymerize the system until the pH value = 5; then add attapulgite, bentonite, 1% sodium sulfite solution, and potassium metabisulfite solution in the polymerization system in a ratio of 1:0.1:0.1:0.01:0.01, and stir evenly after each addition Then add the next raw material; then move the polymerization system into the polymerization reactor, and polymerize at 45°C for 3 hours; finally, dry, pulverize and sieve the polymerized colloid to obtain a multi-component water-retaining agent.
Embodiment 2
[0011] Example 2. First add pure acrylic acid and 1% aqueous solution of N,N'-methylenebisacrylamide in the mixer at a ratio of 1:0.05, and adjust the polymerization system to PH value = 5.5; then add attapulgite, bentonite, 1% sodium sulfite solution, and potassium metabisulfite solution in the polymerization system in a ratio of 1:0.5:0.5:0.02:0.02, and add the following A kind of raw material; then move the polymerization system into the polymerization reactor, and polymerize at 50°C for 3.5 hours; finally, dry, pulverize and sieve the polymerized colloid to obtain a multi-component water-retaining agent.
Embodiment 3
[0012] Example 3. First add 38.5% acrylamide aqueous solution and pure acrylic acid (the ratio of acrylamide aqueous solution to pure acrylic acid is 1:1) and 1% N, N' in the mixer in a ratio of 1:0.1 - methylenebisacrylamide aqueous solution, adjust the polymerization system to PH value = 6 with sodium hydroxide under stirring; then add attapulgite, bentonite, 1% sodium sulfite solution, potassium metabisulfite solution, add the next raw material after stirring evenly each time; then move the polymerization system into the polymerization reactor, and polymerize at 60°C for 4 hours; finally bake the polymerized colloid Drying, crushing, and sieving are multi-component water retaining agents.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com