Preparing method for potassium chloride with low calcium sulfate content
A potassium chloride and product technology, applied in the field of potassium chloride production, can solve problems such as calcium sulfate removal
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The raw materials of bittern and carnallite are taken from Qinghai Chaerhan Salt Lake.
[0026] Get 1000 grams of coarse carnallite and sieve it in saturated brine with a 200-mesh sieve to obtain about 770 grams of carnallite ore on the sieve and about 205 grams of ore on the sieve.
[0027] Take 500 grams of the above-mentioned upper layer of carnallite ore, add it to 2000 grams of saturated brine, stir for about 1 minute, add 0.016 grams of composite flotation agent, stir and mix for 15 minutes, start bubbling flotation for 20 minutes, and then scrape for 15 minutes. After 1 minute, stop the flotation. Filter and weigh the resulting foam layer ore and brine to obtain about 370 grams of lower-layer low-sodium carnallite, with a calcium sulfate content of 0.38%. After the low-sodium carnallite is subjected to a cold crystallization process, potassium chloride products, chlorine Calcium sulfate in potassium chloride is 0.45%.
[0028] The flotation agent is prepared as...
Embodiment 2
[0034] The raw materials of bittern and carnallite are taken from Chaerhan Salt Lake in Qinghai.
[0035] Get 1000 grams of coarse carnallite and sieve it with a 200-mesh sieve in saturated brine to obtain about 770 grams of carnallite ore on the sieve and about 205 grams of ore on the sieve.
[0036] Take 500 grams of the above-mentioned carnallite ore larger than 200 meshes, mix and separate rapidly with 2000 grams of fresh water to obtain about 200 grams of solid particles mainly composed of sodium chloride, potassium chloride and calcium sulfate; mix the resulting mixture with saturated brine Mix evenly at a ratio of 30%, add 500 g of flotation agent per ton of brine, stir for 0.5 hours to obtain about 60 g of potassium chloride particles by flotation, and then further wash, filter, and dry to obtain potassium chloride products, potassium chloride The content of calcium sulfate in the medium is 0.18%.
[0037] The flotation agent is prepared as follows:
[0038] 10wt%C...
Embodiment 3
[0042] The raw materials of bittern and carnallite are taken from Chaerhan Salt Lake in Qinghai.
[0043] Get 1000 grams of coarse carnallite and sieve it with a 200-mesh sieve in saturated brine to obtain about 770 grams of carnallite ore on the sieve and about 205 grams of ore on the sieve.
[0044] Take 500 grams of the above-mentioned upper layer of carnallite ore, add it to 2000 grams of saturated brine, stir for about 1 minute, add 0.016 grams of composite flotation agent, stir and mix for 15 minutes, start bubbling flotation for 20 minutes, and then scrape for 15 minutes. After 1 minute, stop the flotation. Filter and weigh the resulting foam layer ore and brine to obtain about 370 grams of lower-layer low-sodium carnallite, with a calcium sulfate content of 0.38%. After the low-sodium carnallite is subjected to a cold crystallization process, potassium chloride products, chlorine Calcium sulfate in potassium chloride is 0.45%.
[0045] The flotation agent is prepared...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com