Gas for soldering or cutting metals and its preparing method
A technology for welding and cutting gas and metal, used in gas fuel, petroleum industry, fuel and other directions, can solve the problems of welding quality not reaching the level of acetylene gas, difficulty in exerting the effect of additives, shortening the service life of steel cylinders, etc., to achieve good cutting quality, cutting Fast speed, make up for the effect of incomplete gasification
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0026] The preparation method of metal welding and cutting gas: weigh 50 grams of ethylene glycol methyl ether, 20 grams of fusel oil, 10 grams of polyoxyethylene ether surfactant composition, wherein 4 grams of phenylphenol polyoxyethylene ether, alkyl 6 grams of phenol polyoxyethylene ether, 12 grams of 1% ferrocene methanol solution, and 8 grams of 1% diphenylamine methanol solution are mixed to form an additive, and the above-mentioned additive is poured into the air after 0.6% of the gas weight has been removed. 12 liters of steel cylinders are filled with 4 kg of liquefied propylene and propane mixture according to the weight ratio of liquefied propylene: liquefied propane=80:20, which is the metal welding and cutting gas.
example 2
[0028] The preparation method of metal welding and cutting gas: Weigh 40 grams of ethylene glycol methyl ether, 25 grams of fusel oil, and 15 grams of polyoxyethylene ether surfactant composition, of which phenylphenol polyoxyethylene ether 4.2 grams of alkylphenol 10.8 grams of polyoxyethylene ether, 15 grams of 1% ferrocene methanol solution, and 5 grams of 1% diphenylamine methanol solution are mixed to form additives. Get the above additives by 0.8% of the gas weight and pour them into 12 grams after the air has been removed. liter steel cylinder, by the weight ratio of liquefied propylene: liquefied propane=50:50, be filled with 4 kilograms of liquefied propylene, propane mixture and be metal welding and cutting gas.
example 3
[0030] The preparation method of metal welding and cutting gas: Weigh 60 grams of ethylene glycol methyl ether, 15 grams of fusel oil, 5 grams of polyoxyethylene ether surfactant composition, wherein 2.5 grams of phenylphenol polyoxyethylene ether, alkyl 2.5 grams of phenol polyoxyethylene ether, 8 grams of 1% ferrocene methanol solution, and 12 grams of 1% diphenylamine methanol solution are mixed to be additives, and the above-mentioned additives are poured into the gas after 0.4% of the gas weight has been removed. 12 liters of steel cylinders are filled with 4 kg of liquefied propylene and propane mixture in a weight ratio of liquefied propylene: liquefied propane=20:80, which is metal welding and cutting gas.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com