Solid phosphoric acid catalyst for low carbon olefine oligomerization or polymerization
A phosphoric acid catalyst, low-carbon olefin technology, applied in the fields of hydrocarbons, hydrocarbons, organic chemistry, etc., can solve the problems of not achieving high catalytic activity and high strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 2
[0028] According to the preparation method of embodiment 1, difference: replace magnesium oxide with niobium pentoxide, 90 gram boron oxides replace 105 gram boric acid, the solid phosphoric acid catalyst that makes consists of:
[0029] Si 1 B 1.35 Nb 0.08 (P 2 o 5 ) 1.55 ·(H 2 O) 0.8
[0030] Catalyst crush strength 980N / cm 2 .
[0031] According to the aforementioned catalyst evaluation process, the catalyst was used in the butene-2 oligomerization reaction, and the evaluation process conditions were: reaction temperature 180 ° C, pressure 5.0 MPa, liquid volume space velocity 2.0 hours -1 , the raw material butene-2 concentration is 85.8% (mass). Catalyst evaluation results: butene-2 oligomerization was carried out for 80 days, the average conversion rate of butene-2 was 85.0%, and the selectivity of octene was 90.1%. The catalyst liquid yield reached 1700 kg / kg catalyst, and the catalyst activity showed no downward trend. [Example 3]
Embodiment 3
[0032] According to the preparation method of Example 1, difference: 450 grams of polyphosphoric acid, replace magnesium oxide with zirconia and manganese dioxide; Pass into air and water vapor to activate, air: water vapor molar ratio 1.1: 1, activation temperature 200°C, activation time 4 hours, the composition of the prepared solid phosphoric acid catalyst is:
[0033] Si 1 B 0.88 mn 0.03 Zr 0.07 (P 2 o 5 ) 1.40 ·(H 2 O) 0.9
[0034] Catalyst crush strength 900N / cm 2 .
[0035] According to the aforementioned catalyst evaluation process, the catalyst was used in the propylene oligomerization reaction, and the evaluation process conditions were: reaction temperature 190 ° C, pressure 4.0 MPa, liquid volume space velocity 2.0 hours -1 , raw material propylene concentration 47% (mass). The evaluation results of the catalyst were as follows: the propylene oligomerization reaction lasted for 12 days, the average conversion rate of propylene was 79.8%, and ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com