Multifunctional granulated fiber for asphalt mixture road, and preparation method thereof
A kind of asphalt mixture, multi-functional technology, applied in the field of multi-functional granulated fiber for asphalt mixture road and its preparation, can solve the problems of easy agglomeration of steel wool fiber and unfavorable engineering application, so as to improve the reinforcement effect and reduce the time spent , the effect of system stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] A multifunctional granulated fiber for asphalt mixture road,
[0034] (1) average length is 5mm steel wool fiber and brucite fiber dispersion;
[0035] (2) Take raw materials by weighing 90%, 0%, 3.0%, 3.0%, 3.0%, 1.0% by volume ratio of steel wool fiber, brucite fiber, heavy oil, aromatic oil, bentonite, diatomaceous earth;
[0036] (3) Put the weighed raw materials into the mixer and stir evenly, and the mixed raw materials need to stand still in the stuffing bucket for 10-15 minutes;
[0037] (4) Rotate and extrude the rested raw materials with a granulator to obtain multifunctional granulated fibers with a diameter of 4 mm and a length of 0.8 to 1 cm.
Embodiment 2
[0039] A multifunctional granulated fiber for asphalt mixture road,
[0040] (1) average length is 5mm steel wool fiber and brucite fiber dispersion;
[0041] (2) Take raw materials by weighing 72%, 18%, 3.0%, 3.0%, 3.0%, 1.0% by volume ratio of steel wool fiber, brucite fiber, heavy oil, aromatic oil, bentonite, diatomite;
[0042] (3) Put the weighed raw materials into the mixer and stir evenly, and the mixed raw materials need to stand still in the stuffing bucket for 10-15 minutes;
[0043] (4) Rotate and extrude the rested raw materials with a granulator to obtain multifunctional granulated fibers with a diameter of 4 mm and a length of 0.8 to 1 cm.
Embodiment 3
[0045] A multifunctional granulated fiber for asphalt mixture road,
[0046] (1) average length is 5mm steel wool fiber and brucite fiber dispersion;
[0047] (2) Take raw materials by weighing 54%, 36%, 3.5%, 2.5%, 3.0%, 1.0% by volume ratio of steel wool fiber, brucite fiber, heavy oil, aromatic oil, bentonite, diatomaceous earth;
[0048] (3) Put the weighed raw materials into the mixer and stir evenly, and the mixed raw materials need to stand still in the stuffing bucket for 10-15 minutes;
[0049](4) Rotate and extrude the rested raw materials with a granulator to obtain multifunctional granulated fibers with a diameter of 4 mm and a length of 0.8 to 1 cm.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
density | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com