A positive electrode material, high-nickel technology, applied in battery electrodes, structural parts, electrical components, etc., can solve the problems of high cost and damage to the lattice stability of high-nickel materials, and achieve the effect of improving lattice stability and saving costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] With 1000g nickel-cobalt-aluminum molar ratio 88:7:5 particle diameter D50 is the nickel-cobalt-aluminum composite hydroxide precursor of 18um, and 1.81g Mg(OH) 2 And 473g lithium hydroxide monohydrate (molar ratio Li:Me=1.025:1) joins in the small-scale high-speed mixer, unloads after mixing 0.5h, packs in the sagger, burns in oxygen atmosphere 780 ℃ (overburning (calcination temperature 50°C) for 10h, then 500g of one-fired NCA and 2.86g of boron oxide were fired at 250°C for 6h to obtain a high-nickel cathode material A.
[0032] With 1000g nickel-cobalt-aluminum molar ratio 88:7:5 particle diameter D50 is the nickel-cobalt-aluminum composite hydroxide precursor of 2.3um, and 1.81g Mg(OH) 2 And 473g lithium hydroxide monohydrate (molar ratio Li:Me=1.025:1) joins in the small-scale high-speed mixer, unloads after mixing 0.5h, packs in the sagger, burns (overburned at 740 ℃ in oxygen atmosphere) (calcination temperature 40°C) for 10h, and then 500g of one-fired NCA an...
Embodiment 2
[0036] With 1000g nickel-cobalt-aluminum molar ratio 88:7:5 particle diameter D50 is the nickel-cobalt-aluminum composite hydroxide precursor of 18um, and 1.81g Mg(OH) 2 And 473g lithium hydroxide monohydrate (molar ratio Li:Me=1.025:1) joins in the small-scale high-speed mixer, unloads after mixing 0.5h, packs in the sagger, burns in oxygen atmosphere 810 ℃ (overburning (calcination temperature 80°C) for 10h, and then 500g of one-fired NCA and 2.86g of boron oxide were fired at 250°C for 6h to obtain a high-nickel cathode material.
[0037] With 1000g nickel-cobalt-aluminum molar ratio 88:7:5 particle diameter D50 is the nickel-cobalt-aluminum composite hydroxide precursor of 2.3um, and 1.81g Mg(OH) 2 And 473g lithium hydroxide monohydrate (molar ratio Li:Me=1.025:1) joins in the small-scale high-speed mixer, unloads after mixing 0.5h, packs in the sagger, burns in oxygen atmosphere 780 ℃ (overburning (calcination temperature 80°C) for 10h, and then 500g of one-fired NCA and...
Embodiment 3
[0040] With 1000g nickel-cobalt-aluminum molar ratio 88:7:5 particle diameter D50 is the nickel-cobalt-aluminum composite hydroxide precursor of 18um, and 1.81g Mg(OH) 2 And 473g lithium hydroxide monohydrate (molar ratio Li:Me=1.025:1) joins in the small-sized high-speed mixer, unloads after mixing 0.5h, packs in the sagger, burns (overburned at 760 ℃ in oxygen atmosphere) (calcination temperature 30°C) for 10h, and then 500g of one-fired NCA and 2.86g of boron oxide were fired at 250°C for 6h to obtain a high-nickel cathode material A.
[0041] With 1000g nickel-cobalt-aluminum molar ratio 88:7:5 particle diameter D50 is the nickel-cobalt-aluminum composite hydroxide precursor of 2.3um, and 1.81g Mg(OH) 2 And 473g lithium hydroxide monohydrate (molar ratio Li:Me=1.025:1) joins in the small-sized high-speed mixer, unloads after mixing 0.5h, packs in the sagger, burns in oxygen atmosphere 730 ℃ (overburning (calcination temperature 30°C) for 10h, and then 500g of one-fired NC...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com